New techniques for aligning nanocrystals enhance solar-cell efficiency and LED performancesource:RIKENIn a study that unlocks exciting possibilities for solar cells and light-emitting diodes (LEDs) based on materials known as perovskites, RIKEN researchers have refined techniques for controlling the optical and electronic properties of perovskite nanocrystals.The high tunability of all-inorganic nanocrystals made from perovskite materials with the chemical formula CsPbX3 (where X is a halide such as chlorine, bromine or iodine) make them attractive for use in various applications, including bi...
Release time: 2025 - 02 - 28
viewed:42
source:Phys.orgA team of engineers and physicists at Southern University of Science and Technology, in China, has created a nickel-based material that behaves as a superconductor above the -233°C (40 K) threshold under ambient pressure. In their study published in Nature, the researchers synthesized thin films of bilayer nickelate (La₂.₈₅Pr₀.₁₅Ni₂O₇) and found one that behaved as a high-temperature superconductor.The -233°C threshold (40 K), often associated with the McMillan limit, marks a boundary beyond which conventional superconductivity theories become less predictive.Scientist...
Release time: 2025 - 02 - 27
viewed:54
source:Helmholtz Association of German Research CentresCadmium selenide nanoplatelets provide a promising foundation for the development of innovative electronic materials. Researchers around the world have taken a particular interest in these tiny platelets, which are only a few atoms thick, as they offer extraordinary optical and other properties.A team from the Helmholtz-Zentrum Dresden-Rossendorf (HZDR), TU Dresden, and the Leibniz Institute for Solid State and Materials Research Dresden (IFW) has taken an important step toward the systematic production of such nanoplatelets. The researche...
Release time: 2025 - 02 - 26
viewed:50
source:resourceworldAmerican Rare Earths Ltd. [ASX: ARR; OTCQX: ARRNF and AMRRY] reported results of its updated Halleck Creek, Wyoming, Scoping Study, confirming the project’s strong economics, scalability, and strategic importance.Compiled by independent engineering firm Stantec Consulting Services Inc., the Study highlights Halleck Creek’s strong economic potential, strategic advantages, and clear pathway to development as a U.S.-based rare earths project. Located in Wyoming, a Tier 1 mining jurisdiction, Halleck Creek benefits from state land tenure, allowing for accelerated permitting and...
Release time: 2025 - 02 - 25
viewed:47
Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
犀牛云提供云计算服务