Development of rare earth element-based hybrid aluminium composites using stir casting process

The date of: 2024-11-15
viewed: 3
source:Scientific Reports


Abstract
Aerospace and marine industries are constantly in search of materials that can provide good strength and durability while also being lightweight. Aluminium composites with adequate reinforcements have been proven to be effective in achieving incredible mechanical properties while also maintaining a good strength to weight ratio. Numerous studies have been done to study the various possibilities of matrix reinforcement combinations in aluminium composites. This work focuses on studying the effect of varying Cerium Oxide (CeO2) percentage in the aluminium composite on its tensile strength, hardness and corrosion resistance. CeO2 is used along with Silicon Carbide (SiC) and Multi-Walled Carbon Nanotubes (MWCNT) to develop four samples of hybrid aluminium composites with SiC and MWCNT constituting 1% and 0.1% of the composite and the weight percentage of CeO2 is varied between 1 and 2.5%. All the samples were fabricated using the modified stir casting process. The results show that the hardness and tensile strength of the composites peak when the CeO2% is at 2% while corrosion resistance only gets better with increasing reinforcement content. A significant enhancement in mechanical and physical properties of aluminium composite suggests that MWCNT is an effective hybridizing agent with SiC and CeO2 to develop aluminium composites.



Hot News / Related to recommend
  • 2025 - 11 - 17
    Click on the number of times: 2
    来源:ACS PublicationsThis work reports the fabrication of a novel electrochemical sensor leveraging reduced graphene oxide (rGO) modified with samarium oxide (Sm2O3) nanoparticles to enhance dopamine (D...
  • 2025 - 11 - 14
    Click on the number of times: 0
    Manipulating Local Electron Density of Fe Nanoclusters with Cerium Incorporation to Optimize Adsorption Behavior of N-Related Intermediates for Electrochemical Ammonia Synthesis from Nitrite来源:ACS Pub...
  • 2025 - 11 - 14
    Click on the number of times: 0
    Bi-, Tri- and Tetranuclear Rare Earth Metal Complexes with Arylboronic Acids: Synthesis, Structure, and Photoluminescent Properties来源:ACS PublicationsPolynuclear complexes of rare earth metals Sc, La,...
  • 2025 - 11 - 12
    Click on the number of times: 2
    Ultrathin Single-Helix Rare Earth Nanowires: Inorganic Analogues of RNA Conformation with High Mechanical Flexibility来源:ACS PublicationsChirality has always been fascinating, yet inorganic chiral stru...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务