Anionic Condensation-Guided Synthesis of LaSi2N3O: A “Missing” Structure in the Ln–Si–N–O Series of Oxonitridosilicate Phosphor Materials

The date of: 2026-05-26
viewed: 15

来源:ACS Publications

The development of innovative luminescent materials for lighting and display applications is an important research field. In this work, we have employed an anionic condensation approach to discover a novel oxonitridosilicate synthesized via Li metal flux. LaSi2N3O crystallizes in the orthorhombic space group Pna21 (a = 7.82609(6), b = 18.24908(15), and c = 4.86567(5) Å) with a structure consisting of [Si6N12O2] ribbons cross-linked by [SiN3O] tetrahedra. This follows previously reported structural rules for a series of condensed rare-earth oxonitridosilicates, and discovery of this relatively simple composition verifies the design principles. Ce3+-doped LaSi2N3O is a highly efficient blue phosphor with peak emission at 450 nm under 390 nm excitation and a quantum yield of 72.0% and demonstrates strong potential for near-UV phosphor applications.


Hot News / Related to recommend
  • 2026 - 11 - 20
    Click on the number of times: 7
    来源:Nature CommunicationsEfficient 1.54 µm electroluminescence from erbium ions has long been hindered by their intrinsically small absorption cross-section and low excitation efficiency in conven...
  • 2026 - 11 - 19
    Click on the number of times: 5
    来源:Nature CommunicationsDry reforming of methane (DRM) with carbon dioxide produces CO-rich syngas for methanol and Fischer–Tropsch fuel synthesis, but carbon deposition deactivates catalysts and limi...
  • 2026 - 11 - 18
    Click on the number of times: 8
    来源:Nature CommunicationsSpatial-light computing requires rewritable, multilevel and persistent optical weights, but many implementations rely on volatile modulators or static power. Here we report a C...
  • 2026 - 11 - 17
    Click on the number of times: 9
    来源:Nature CommunicationsLanthanide-doped upconversion nanoparticles exhibit multicolor emission through discrete, narrowband transitions, enabling applications in bioimaging, lasers, and displays. How...