Defect-Driven Optical Modulation in Rare-Earth-Modified Zn2SnO4 Spinels for Advanced Optoelectronic Applications

The date of: 2026-05-27
viewed: 0

来源:ACS Publications

Spinel-type Zn2SnO4 and its La- and Ce-modified variants were synthesized via a solid-state route to investigate aliovalent substitution–induced structural, optical, and photoluminescence (PL) modulation. Undoped, La- and Ce-doped Zn2SnO4 samples were characterized using X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, Raman spectroscopy, ultraviolet–visible spectroscopy, photoluminescence, scanning electron microscopy (SEM)–energy-dispersed spectroscopy (EDS), and X-ray photoelectron spectroscopy (XPS) techniques. XRD confirmed the dominant cubic spinel structure (Fd3̅m:1) with a minor SnO2 phase, while rare-earth incorporation induced lattice expansion, microstrain, and reduced crystallite size (32–27 nm). FTIR, Raman, and XPS analyses revealed dopant-induced lattice distortion, enhanced oxygen-vacancy-related defects, and the presence of Zn2+, Sn4+, La3+, and mixed Ce3+/Ce4+ states. Optical studies showed band gap narrowing from 3.57 eV (undoped) to 3.16 eV (La-doped) and 3.12 eV (Ce-doped), extending visible-light activity. PL results demonstrated dopant-selective color tunability, with orange emission for La-doped and green emission for Ce-doped Zn2SnO4. These findings establish a clear structure–defect–optical correlation and highlight rare-earth-modified Zn2SnO4 as a promising material for visible-light optoelectronic, luminescence, and optical sensing applications.


Hot News / Related to recommend
  • 2026 - 07 - 17
    Click on the number of times: 0
    Hybrid Solvation Model for Analyzing the Binding of Yttrium and Calcium Cations to the Lanmodulin Protein Using the Fragment Molecular Orbital Method 来源:ACS PublicationsA hybrid solvation model combin...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsChemically flexible A2B2O7 oxides are attractive candidates for designing structure-specific functional materials by judicious substitution. However, modulating functionality by sub...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsRational design of Eu2+-activated red phosphors under visible light excitation remains a critical challenge in various fields such as photonics, optoelectronics, and white-light-emi...
  • 2026 - 07 - 15
    Click on the number of times: 0
    来源:ACS PublicationsPolaron formation has emerged as an important mechanism for unconventional luminescence in metal halide semiconductors. Here, we show that incomplete rare-earth-ion doping in the ze...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务