Rare earth oxide prices mostly rose on improved demand on week

The date of: 2019-12-03
viewed: 1

source:SMM - Shanghai Metals Market (press release)

Prices of rare-earth oxides in China, except for lanthanum oxide and cerium oxide, were in an upward trend last week, supported by improved trades in the spot market. 

SMM assessments indicated that, as of December 2, dysprosium oxide prices climbed to 1.63-1.65 million yuan/mt, from 1.6-1.62 million yuan/mt last Monday; prices of terbium oxide held stable at 3.4-3.45 million yuan/mt last week and gained 10,000 yuan/mt on Monday December 2. 

Prices of praseodymium-neodymium oxide, meanwhile, relinquished early gains last week and stood at 283,000-286,000 yuan/mt as of December 2, flat from a week ago. 

SMM assessed prices of dysprosium-ferrum alloy at 1.62-1.64 million yuan/mt as of December 2, up from 1.59-1.61 million yuan/mt a week earlier.

Downstream metal and magnetic material producers will likely step up restocking ahead of the Chinese New Year, but growth in overseas consumption before the upcoming Christmas holiday could be limited. 

There is potential upside room in prices of light rare earth, such as praseodymium-neodymium oxide and neodymium oxide, on the back of rising demand even as supply will expand on higher production quotas. 

Near-term prices of medium- to heavy- rare earth, including dysprosium oxide and terbium oxide, may also extend increase as major producers firm up offers amid the prospect of demand recovery. 



Hot News / Related to recommend
  • 2025 - 07 - 14
    Click on the number of times: 0
    Compensation-Like Temperature and Spin-Flip Switch in Strained Thulium Iron Garnet Thin Films: Tuning Sublattice Interactions for Ferrimagnetic Spintronics 来源:ACS PublicationsCertain rare-earth i...
  • 2025 - 07 - 10
    Click on the number of times: 0
    Computational Investigations of Metal–Metal Bonding in Molecular Thorium Compounds and Ce and Group IV Analogues来源:ACS PublicationsWe report quantum chemical investigations of metal–metal bonding in m...
  • 2025 - 07 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe reaction between isophthalic acid (H2L1) and Gd(NO3)3·6H2O leads to the formation of a two-dimensional (2D) extended framework with the molecular formula [Gd2(L1)3(H2O)2]n ...
  • 2025 - 07 - 08
    Click on the number of times: 0
    来源:ACS PublicationsA straightforward synthesis of Cp*2Sc(AlMe4) (Cp* = C5Me5) applying Cp*2ScCl(thf) and LiAlMe4/AlMe3 is described. Donor-assisted trimethyltriel exchange gives access to Cp*2Sc(EMe4)...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务