Rare-Earth Hafnium Molybdates A Structural, Optical, and Magnetic Study

The date of: 2026-07-28
viewed: 6

来源:ACS Publications

The molten flux method was used to grow crystals belonging to two different classes of rare-earth hafnium molybdates, RE2Hf3(MoO4)9 and RE2Hf2(MoO4)7, whose luminescence and magnetic properties were investigated. The first structure type, RE2Hf3(MoO4)9, spans from La to Eu (except Pm) and crystallizes in the trigonal R-3c space group. In this structure, MoO4, REO9, and HfO6 are connected via their corners. The MoO4 units form open channels along the c-axis, which are occupied by columns of REO9 and HfO6 polyhedra. The second structure type, RE2Hf2(MoO4)7, includes RE = Sm, Eu, Gd, Tb, and Dy and crystallizes in the monoclinic C2/c space group. The MoO4 tetrahedra connect through their corners to HfO6 octahedra and DyO8 square antiprisms, forming a three-dimensional open framework. Magnetic and photoluminescence properties were measured on polycrystalline samples obtained from solid-state reactions. Eu2Hf3(MoO4)9 and Tb2Hf2(MoO4)7 exhibit photoluminescence under UV irradiation. Eu(III) was doped successfully into La2Hf3(MoO4)9 and characterized by single-crystal X-ray diffraction and single-crystal photoluminescence emission spectroscopy. Magnetic susceptibility vs temperature measurements were performed to investigate the magnetic behavior of Ce2Hf3(MoO4)9, Gd2Hf2(MoO4)7, and Dy2Hf2(MoO4)7.


Hot News / Related to recommend
  • 2026 - 09 - 16
    Click on the number of times: 0
    来源:ACS PublicationsSurface plasmons modulate rare-earth luminescence via local field enhancement and photothermal effects, yet the synergy-competition between these inherently coupled effects remains ...
  • 2026 - 09 - 15
    Click on the number of times: 0
    Phytogenic Self-Conducting Flash Joule Heating Converts Rare-Earth Hyperaccumulator Biomass into Graphene Composites with Minimized Life-Cycle Impacts 来源:ACS PublicationsRare-earth elements (REEs) are...
  • 2026 - 09 - 15
    Click on the number of times: 0
    来源:ACS PublicationsSecuring a sustainable supply of rare earth elements (REEs) requires efficient separation and recovery from secondary streams. Zeolites are attractive, low-impact sorbents; however,...
  • 2026 - 09 - 14
    Click on the number of times: 0
    Detoxification of Ion-Adsorption Rare Earth Elements Low-Level Radioactive Residues via Mild Alkali–Carbonate: Uranium Extraction and Multi-Metal Recovery 来源:ACS PublicationsImpeded by the harsh high-...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务