A Study on the Synergistic Adsorption Performance of ZIF-8/HKUST-1 Nanocomposite for La3+ Ions

The date of: 2026-05-13
viewed: 14

来源:ACS Publications

In this study, ZIF-8/HKUST-1 and ZIF-67/HKUST-1 composite materials were fabricated via a stepwise solvent-assisted synthesis route. The materials were characterized by Fourier-transform infrared spectroscopy (FT-IR), X-ray diffraction (XRD), scanning electron microscopy (SEM), and N2 physisorption (BET). The La3+ adsorption performance was systematically evaluated through batch experiments under varying pH, contact time, initial concentration, and temperature. The experimental data were fitted to kinetic, isotherm, and thermodynamic models to elucidate the underlying adsorption mechanism. ZIF-8/HKUST-1 showed the best performance for La3+ adsorption using a pH of 6. Under this condition, adsorption equilibrium was attained in just 30 min, and the maximum adsorption capacity reached 250.72 mg/g. The composite also maintained 81.25% of its initial capacity after five adsorption–desorption cycles. This excellent retention rate attests to its structural stability and reusability, pointing to a strong potential for industrial use.



Hot News / Related to recommend
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe integration of diverse electronic phenomena, such as magnetism and nontrivial topology, into a single low-dimensional system gives rise to unusual quantum effects. Here we combi...
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth elements (REEs: La–Lu, Y, Sc) are critical to modern technology; however, their acquisition, purification, and separation from each other can be challenging, and current ...
  • 2026 - 10 - 08
    Click on the number of times: 0
    来源:ACS PublicationsThe synthesis of alkali-metal-free compounds [LnMe3]n is scrutinized using two distinct protocols. The donor-promoted cleavage of homoleptic tetramethylaluminate complexes Ln(AlMe4)...
  • 2026 - 09 - 30
    Click on the number of times: 0
    来源:ScienceDirectIn the in-situ leaching of ionic rare earth ores, ineffective through-flow induced by ore body heterogeneity and suboptimal rinsing strategies constrain both extraction efficiency and ...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务