Monolithic Integration of Rare-Earth-Doped Tellurite Thin Films with Silicon for Dual-Function Optical

The date of: 2026-04-03
viewed: 15

来源:ACS Publications

For next-generation applications, recent developments in sensor fabrication technologies and innovative materials have rendered improved temporal response and spectral detection capabilities feasible. This work demonstrates a dual-mode sensor for simultaneous light and temperature detection. Vacuum thermal evaporation was used to deposit nanostructured polycrystalline TeO2–Li2O–ZnO–Nb2O5–Dy2O3 (TLZND) thin films (∼32 nm crystallites) on monolithic substrates. Field-emission scanning electron microscopy revealed surface morphology and roughness, while Fourier transform infrared spectroscopy described postevaporation molecular structural changes. Optical characteristics, such as energy gap and dispersion parameters, were determined using UV–vis–near-IR spectroscopy. Dark direct-current conductivity showed three different activation energy regions, increasing from 6.33 × 10–5 to 2.14 × 10–3 Ω–1 cm–1. Three sensitivity regions with different linearities were shown by silicon-integrated TLZND heterojunctions between 303 and 473 K. Effective dual-mode sensing capability was confirmed by the sensor’s fast response to halogen and multiwavelength laser radiation, which resulted in optimal infrared performance: 7.44 A/W responsivity, 6.82 × 1010 Jones detectivity, and 40 ms response time.


Hot News / Related to recommend
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe integration of diverse electronic phenomena, such as magnetism and nontrivial topology, into a single low-dimensional system gives rise to unusual quantum effects. Here we combi...
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth elements (REEs: La–Lu, Y, Sc) are critical to modern technology; however, their acquisition, purification, and separation from each other can be challenging, and current ...
  • 2026 - 10 - 08
    Click on the number of times: 0
    来源:ACS PublicationsThe synthesis of alkali-metal-free compounds [LnMe3]n is scrutinized using two distinct protocols. The donor-promoted cleavage of homoleptic tetramethylaluminate complexes Ln(AlMe4)...
  • 2026 - 09 - 30
    Click on the number of times: 0
    来源:ScienceDirectIn the in-situ leaching of ionic rare earth ores, ineffective through-flow induced by ore body heterogeneity and suboptimal rinsing strategies constrain both extraction efficiency and ...