Localized Excitonic Magnetic Polarons and Their Role in the Luminescence of Rare-Earth-Sulfur Codoped Divalent Metal Halides

The date of: 2026-03-25
viewed: 20

来源:ACS Publications

In this work, BaCl2:Eu2+,S2– is employed as model system to investigate the formation and tunable evolution of localized excitonic magnetic polarons (LEMPs) in Eu–S codoped divalent metal halides, in which Eu–S bonding in BaCl2 with Eu2+ 5d–f hybridization markedly enhances the band edge emission, shifting from 401 to 412 nm with rising EuS content, and the absorption band edge shifts from 3.02 to 2.85 eV, with EMP character. Moreover, EuS doped in different hosts (Ba < Sr < Ca) leads to a progressive red shift of EMP emission from 406 nm to the near-infrared region. Under high-energy laser excitation, these compounds can exhibit pronounced nonlinear emission with ASE-like behavior (n > 1), demonstrating the LEMP-cooperative radiative processes. This study establishes rare-earth-sulfur codoped halides as a promising materials platform for tuning luminescence through coupled spin–lattice–exciton interactions.


Hot News / Related to recommend
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe integration of diverse electronic phenomena, such as magnetism and nontrivial topology, into a single low-dimensional system gives rise to unusual quantum effects. Here we combi...
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth elements (REEs: La–Lu, Y, Sc) are critical to modern technology; however, their acquisition, purification, and separation from each other can be challenging, and current ...
  • 2026 - 10 - 08
    Click on the number of times: 0
    来源:ACS PublicationsThe synthesis of alkali-metal-free compounds [LnMe3]n is scrutinized using two distinct protocols. The donor-promoted cleavage of homoleptic tetramethylaluminate complexes Ln(AlMe4)...
  • 2026 - 09 - 30
    Click on the number of times: 0
    来源:ScienceDirectIn the in-situ leaching of ionic rare earth ores, ineffective through-flow induced by ore body heterogeneity and suboptimal rinsing strategies constrain both extraction efficiency and ...