Observation of Microscopic Domain Effects in the Metal–Insulator Transition of Thin-Film NdNiO3

The date of: 2026-03-20
viewed: 15

来源:ACS Publications

Perovskite oxides display correlated electrical, magnetic, and thermal properties that can be further tuned in the thin-film limit, making them contenders for next-generation electronics. Measuring thermal transport in thin films is challenging, because traditional techniques are dominated by the substrate. Here, frequency-domain thermoreflectance (FDTR) of an epitaxial NdNiO3 thin film reveals a sharp change in out-of-plane thermal conductivity across the metal–insulator transition. Complementary frequency-domain photoreflectance (FDPR) reveals a large change in ambipolar diffusivity of photoexcited carriers. While the in-plane electrical resistance shows large hysteresis, out-of-plane thermal and charge transport shows negligible hysteresis. We attribute this discrepancy to anisotropy in the percolation of nanoscale domains across the transition as the film thickness approaches the domain length scale. We establish FDTR and FDPR as sensitive probes of quantum material phase transitions and highlight NdNiO3 for thermal control and memory applications.



Hot News / Related to recommend
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsIron (Fe)-rich tailings generated during rare earth element (REE) processing constitute a strategically important secondary resource. However, their utilization is hindered by the r...
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsHigh-entropy rare-earth oxides (HE-REOs) offer a broad compositional space for tuning defect chemistry, lattice distortion, and local atomic environments, yet their controlled synth...
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsSeparation of Rare Earth Elements (REEs) remains an open challenge for their closely related coordination chemistry and hydration. Neodymium (Nd) and yttrium (Y) form an exemplary p...
  • 2026 - 09 - 03
    Click on the number of times: 2
    The Synergistic Impact of Lanthanide-Doped Nickel Iron Sulphides (NiFeSs) Synthesized by a Hydrothermal Method for Effective Water and Urea Electrolysis in Anion Exchange Membranes来源:ACS PublicationsO...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务