Growth and Enhancement of Magneto-Optical Properties in the Dysprosium-Doped Large-Size Yttrium Iron Garnet Crystal

The date of: 2026-01-30
viewed: 16

来源:ACS Publications

The growing demand for nonreciprocal optical devices has intensified the need for high-performance magneto-optical materials. Yttrium iron garnet (YIG) stands out for its excellent magnetic and magneto-optical characteristics. In this work, centimeter-sized dysprosium-doped YIG single crystals were successfully synthesized via the top-seeded solution growth method. The integration of Dy3+ ions significantly reduces both coercivity and saturation magnetization compared with pure YIG, enabling magnetic saturation under lower external fields. The as-grown crystal exhibits ferrimagnetic behavior with a saturation magnetization of 9.96 emu/g and a coercivity of 8.40 Oe. Postgrowth oxygen annealing effectively suppresses Fe2+ and oxygen vacancy defects, further improving the magneto-optical performance. After annealing at 900 °C, the defect concentration is minimized, leading to a reduced coercivity of 5.09 Oe. Moreover, the treated crystal shows enhanced optical transmittance (71.93% at 1550 nm, 76.05% at 2000 nm), and the Faraday rotation angle increased by more than 12% (184°/cm at 1550 nm, 123°/cm at 2000 nm). These results highlight the essential role of oxygen annealing in optimizing crystal quality and magneto-optical functionality, thus providing critical insights for the property design and postprocessing of magneto-optical materials.


Hot News / Related to recommend
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsSiloxane and aluminol surfaces, ubiquitous in Earth’s system, regulate the adsorption of economically vital elements such as rare earth elements (REEs), yet their atomic-scale react...
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth-doped glasses have great potential in magneto-optical applications due to their high transparency and Verdet constant. However, their synthesis not only requires a high-t...
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsStrong demand for rubber, coupled with limited natural rubber supply, has accelerated the development of synthetic alternatives. Metal-catalyzed polymerization is a key route to hig...
  • 2026 - 05 - 13
    Click on the number of times: 1
    来源:ACS PublicationsIn this study, ZIF-8/HKUST-1 and ZIF-67/HKUST-1 composite materials were fabricated via a stepwise solvent-assisted synthesis route. The materials were characterized by Fourier-tran...