Enhanced Piezoelectricity, Coercive Field, and Electrostrain in Sm-Doped Pb(Zn1/3Nb2/3)O3–PbTiO3 Ferroelectric Crystals

The date of: 2025-11-19
viewed: 8

来源 :ACS Publications

Relaxor ferroelectrics with a large piezoelectric coefficient (d33), sizable coercive field (EC), and high signal piezoelectric coefficient (d33*) are of particular importance in technology. Due to the trade-off between domain switching and high energy barriers, materials of this kind are rather rare, and the discovery and design of such materials remain a challenging task. Here, we successfully grew Sm0.01Pb0.985[(Zn1/3Nb2/3)0.93Ti0.07]O3 (Sm–PZN–PT) crystals with a high d33 value of 2930 pC/N (up to 3032 pC/N at 150 °C) and a significantly enhanced EC value of 12.3 kV/cm, representing a 100% improvement compared with previously reported Sm–PZN–PT crystals. The large signal piezoelectric coefficient (d33*) values reached 5130 pm/V. Notably, it exhibits remarkable thermal stability with <2% piezoelectric performance fluctuation up to 150 °C. Through multiscale structural analyses, we have elucidated the enhancement mechanisms governing the respective indexes. This rare-earth doping paradigm opens new avenues for developing high-performance ferroelectrics with exceptional field tolerance and multifunctional integration capabilities.



Hot News / Related to recommend
  • 2026 - 01 - 15
    Click on the number of times: 0
    来源:ACS PublicationsThe binding of rare earth elements to extractants is a key step in their separation and purification by solvent extraction. Classical MD simulations are used to investigate the equi...
  • 2026 - 01 - 14
    Click on the number of times: 0
    来源:ACS PublicationsBisphenol A (BPA) poses significant risks to human health and ecosystems due to its severe adverse effects. Consequently, effective BPA removal from water sources is imperative. Whi...
  • 2026 - 01 - 14
    Click on the number of times: 0
    来源:ACS PublicationsOrganic dyes are commonly used in the textile and leather industries and are frequently detected in natural water bodies, posing potential hazards to the ecological environment and ...
  • 2026 - 01 - 13
    Click on the number of times: 1
    来源:ACS PublicationsHigh-pressure synthesis provides unique pathways to materials with unprecedented structures and properties. Here we report the synthesis and structural characterization of novel rar...