Engineering Trap Distribution by Doping Rare Earth

The date of: 2025-04-17
viewed: 54

Engineering Trap Distribution by Doping Rare Earth Ion for Mechanoluminescence Enhancement

 

Mechanoluminescence materials exhibit fascinating optical properties due to their energy harvesting and controllable release capabilities. SrAl2O4:Eu2+ (SAOE) has been extensively studied as a traditional mechanoluminescence material, however, the luminescence intensity enhancement and the luminescence mechanism of its mechanoluminescence remain an unresolved issue, which hinders the development and widespread application of excellent phosphors. Herein, a promising rare earth (Re3+ = Sm3+, Dy3+, Er3+, and Tm3+) doping strategy was proposed to achieve intense strategy was proposed to achieve intense mechanoluminescence of SAOE. By introducing different Re3+ ions to manipulate the energy level positions in SAOE phosphors, the depth and density of electron and hole traps can be tuned, resulting in the maximum mechanoluminescence intensity of SrAl2O4:Eu2+, Tm3+ is about 11-fold higher than that of SAOE. The mechanism governing trap distribution has been unveiled through thermoluminescence glow curve analysis and density functional theory calculations. Our research provides valuable guidance for designing high-performance phosphors and opens up new opportunities for multifunctional applications.




Hot News / Related to recommend
  • 2026 - 09 - 16
    Click on the number of times: 0
    来源:ACS PublicationsSurface plasmons modulate rare-earth luminescence via local field enhancement and photothermal effects, yet the synergy-competition between these inherently coupled effects remains ...
  • 2026 - 09 - 15
    Click on the number of times: 0
    Phytogenic Self-Conducting Flash Joule Heating Converts Rare-Earth Hyperaccumulator Biomass into Graphene Composites with Minimized Life-Cycle Impacts 来源:ACS PublicationsRare-earth elements (REEs) are...
  • 2026 - 09 - 15
    Click on the number of times: 0
    来源:ACS PublicationsSecuring a sustainable supply of rare earth elements (REEs) requires efficient separation and recovery from secondary streams. Zeolites are attractive, low-impact sorbents; however,...
  • 2026 - 09 - 14
    Click on the number of times: 0
    Detoxification of Ion-Adsorption Rare Earth Elements Low-Level Radioactive Residues via Mild Alkali–Carbonate: Uranium Extraction and Multi-Metal Recovery 来源:ACS PublicationsImpeded by the harsh high-...