Nanopore discrimination of rare earth elements

The date of: 2025-02-17
viewed: 26
source:Nature Nanotechnology


Rare earth elements (REEs), including scandium, yttrium and lanthanides, are strategic resources with unique electric, luminescent and magnetic properties. However, owing to their highly similar physiochemical properties, the identification and separation of all REEs are challenging. Here a Mycobacterium smegmatis porin A nanopore is engineered to contain a nitrilotriacetic acid ligand at its pore constriction. By the further introduction of a secondary ligand Nα,Nα-bis(carboxymethyl)-L-lysine hydrate (ANTA), a dual-ligand sensing strategy was established. A unique property of this strategy is that a variety of REE(III) ions report characteristic blockage features containing three-level transitions, which are critical in discriminating different REE(III)s. The nanopore events of REE(III)s also demonstrate a clear periodicity, suggesting the observation of the lanthanide contraction effect at a single-molecule regime. Assisted by machine learning, all 16 naturally occurring REE(III)s have been identified by the nanopore with high accuracy. This sensing strategy is further applied in analysing bastnaesite samples, suggesting its potential use in geological exploration.



Hot News / Related to recommend
  • 2026 - 04 - 09
    Click on the number of times: 1
    来源:ACS PublicationsCuprous oxide semiconductors have been growing in research interest because of their promising optical and catalytic properties for solar energy conversion. While much recent resear...
  • 2026 - 04 - 08
    Click on the number of times: 2
    来源:ACS PublicationsWe propose to probe the d–f exchange interaction by measuring the response of the itinerant states to an external magnetic field. Two rare-earth monotellurides, TmTe and GdTe, are c...
  • 2026 - 04 - 07
    Click on the number of times: 2
    来源:ACS PublicationsThe electrochemical production of hydrogen peroxide (H2O2) through the two-electron oxygen reduction reaction (2e– ORR) is a sustainable and practical approach that enables efficien...
  • 2026 - 04 - 07
    Click on the number of times: 1
    来源:ACS PublicationsCerium copper oxytelluride (CCOT) and lanthanum copper oxytelluride (LCOT) nanomaterials have been synthesized through a straightforward hydrothermal route to explore their potentia...