Room-Temperature Ferroelectricity and Data Storage Potential in Tellurium Nanowires

The date of: 2024-12-03
viewed: 38
source:TOHOKU UNIVERSITY


A groundbreaking discovery by an international team of scientists has revealed room-temperature ferroelectric and resistive switching behaviors in single-element tellurium (Te) nanowires, paving the way for advancements in ultrahigh-density data storage and neuromorphic computing.
Published in Nature Communications, this research marks the first experimental evidence of ferroelectricity in Te nanowires, a single-element material, which was previously predicted only in theoretical models.
"Ferroelectric materials are substances that can store electrical charge and keep it even when the power is turned off, and their charge can be switched by applying an external electric field - a characteristic essential for non-volatile memory applications," points out co-corresponding author of the paper Professor Yong P. Chen, a principal investigator at Tohoku University's Advanced Institute for Materials Research (AIMR) and a professor at Purdue and Aarhus Universities.
Polar structure and ferroelectric polarization. ©Jinlei Zhang, Jiayong Zhang, Yaping Qi et al.
While ferroelectricity is common in compounds, single-element materials like Te rarely exhibit this behavior due to their symmetric atomic structures.
However, Chen and his colleagues demonstrated that Te nanowires exhibit robust ferroelectric properties at room temperature, thanks to the unique atomic displacement within their one-dimensional chain structure. The discovery was made using piezoresponse force microscopy (PFM) and high-resolution scanning transmission electron microscopy.
uilding on this discovery, the team developed a novel device--a self-gated ferroelectric field-effect transistor (SF-FET) - which integrates both ferroelectric and semiconducting properties in a single device. The SF-FET demonstrates exceptional data retention, fast switching speeds of less than 20 nanoseconds, and an impressive storage density exceeding 1.9 terabytes per square centimeter.
Ferroelectric hysteresis and domain switching. ©Jinlei Zhang, Jiayong Zhang, Yaping Qi et al.
"Our breakthrough opens up new opportunities for next-generation memory devices, where Te nanowires' high mobility and unique electronic properties could help simplify device architectures," says Yaping Qi, an assistant professor at AIMR and co-first author of the study. "Our SF-FET device could also play a crucial role in future artificial intelligence systems, enabling neuromorphic computing that mimics human brain function. Additionally, the findings can help lead to lower power consumption in electronic devices, addressing the need for sustainable technology."
Currently, the team at AIMR, which comprises Qi and Chen, is exploring new 2D, ferroelectric materials using artificial intelligence (AI) techniques, in collaboration with Professor Hao Li's group. This could lead to the discovery of more materials with promising ferroelectric properties or further applications beyond memory storage, such as neuromorphic computing.



Hot News / Related to recommend
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsSiloxane and aluminol surfaces, ubiquitous in Earth’s system, regulate the adsorption of economically vital elements such as rare earth elements (REEs), yet their atomic-scale react...
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth-doped glasses have great potential in magneto-optical applications due to their high transparency and Verdet constant. However, their synthesis not only requires a high-t...
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsStrong demand for rubber, coupled with limited natural rubber supply, has accelerated the development of synthetic alternatives. Metal-catalyzed polymerization is a key route to hig...
  • 2026 - 05 - 13
    Click on the number of times: 1
    来源:ACS PublicationsIn this study, ZIF-8/HKUST-1 and ZIF-67/HKUST-1 composite materials were fabricated via a stepwise solvent-assisted synthesis route. The materials were characterized by Fourier-tran...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务