Korean Institute of Rare Metals produces rare earth permanent magnets from ASM’s NdFeB

The date of: 2021-02-18
viewed: 12

source:Powder Metallurgy Review magazine

The Korean Institute of Rare Metals (KIRAM) has successfully produced and tested 2 kg of pre-sintered permanent magnets, produced with high-purity NdFeb powder from a Korean pilot plant owned by Australian Strategic Materials (ASM)’s, headquartered in Burswood, Australia.

The KIRAM scientists made a strip-cast sample using 5 kg of ASM’s NdFeB powder. The strip was subsequently examined with scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS) in order to confirm the microstructure and magnetic orientation.

Some of the Ziron Tech NdFeB alloy was also pressed into a 2 kg block in order to measure the magnetic characteristics using vibrating sample magnetometry (VSM) compared with a similar sample made from a commercially available alloy.

KIRAM has stated the results indicated that ASM’s pre-sintered magnet exhibited superior magnetic properties than the commercial sample, indicating ASM’s NdFeb alloy is suitable for the production of rare earth permanent magnets. ASM hopes this will prove a further step in its goal of becoming an independent, fully-integrated ‘mine to manufacturer’ producer of critical metals.

“We now have confirmation of the quality and high purity of the permanent magnet alloy and titanium powders ASM can deliver to the Korean industry and, eventually, the global markets,” stated David Woodall, ASM Managing Director. “ASM is now planning to advance in the next few months with the detailed engineering, incorporating both the recently produced titanium and, now, the permanent magnet powders as part of an initial 5,200 tonnes per year plant in Korea, projected to be fully operational by mid-2022.”

Woodall concluded, “The excellent support and collaborative work between the Ziron Tech and KIRAM teams delivered a truly significant result. It provides ASM with confidence that our integrated business model – from the Dubbo Project to metals production – can play an important part in the Korean Government’s ‘New Green Deal’.”



Hot News / Related to recommend
  • 2025 - 07 - 18
    Click on the number of times: 0
    来源:ACS PublicationsWater electrolysis has emerged as a promising pathway for sustainable energy production, highlighting the need for innovative nonprecious bimetallic nanocatalysts to enhance overall...
  • 2025 - 07 - 17
    Click on the number of times: 0
    来源:ACS PublicationsThe growth of high-entropy alloy (HEA) thin films using the molecular beam epitaxy (MBE) technique widens our horizons in materials design. This technique offers precise control of ...
  • 2025 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsDeterministic control of the layering configuration of two-dimensional quantum materials plays a central role in studying their emergent electronic properties. Here we demonstrate i...
  • 2025 - 07 - 15
    Click on the number of times: 0
    来源:ACS Publications Designing functional materials is a promising route to enhance modern technologies. Here, an unreported hexagonal perovskite, LuGaO3, is successfully synthesized in thin-film form,...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务