Fully Suppressed Superconductivity in Nonferromagnetic Heavy Fermion/Superconductor Bilayers: Rocksalt-Type CeO/LaO

The date of: 2026-07-14
viewed: 4

来源:ACS Publications

Superconductor/ferromagnet heterostructures have been investigated extensively because of their capability to break superconducting electron pairs. In this study, we report on heterostructures of a superconductor and heavy-fermion system as an alternative platform for a strong pair-breaking proximity effect. We fabricated rocksalt-type CeO/LaO heteroepitaxial bilayers, where LaO is a superconductor and CeO is a nonferromagnetic heavy-fermion system. While LaO(9.5–21 nm) thin films showed superconductivity below 4.4–5.2 K, the CeO(4.8–5.8 nm)/LaO(9.2–17 nm) bilayers showed no trace of superconductivity down to 0.025 K. This result demonstrates a strong pair-breaking effect at the superconductor/heavy-fermion system heteroepitaxial interface. This effect would provide a useful platform for superconducting micro and nano devices.



Hot News / Related to recommend
  • 2026 - 08 - 11
    Click on the number of times: 0
    来源:ACS PublicationsIn recent years, coal fly ash (CFA) has emerged as a sustainable alternative resource for rare-earth elements (REEs). Acid leaching enables efficient REE recovery, yet large-scale p...
  • 2026 - 08 - 11
    Click on the number of times: 0
    来源:ACS PublicationsThe sustainable separation of rare earth elements (REEs) from complex mixtures remains a critical technological challenge. Biomaterials offer a promising route, but their deployment...
  • 2026 - 08 - 10
    Click on the number of times: 0
    来源:ACS PublicationsThe advancement of polymer electrolyte fuel cells (PEFCs) relies on materials capable of enhancing electrochemical performance while maintaining long-term operational stability. Rar...
  • 2026 - 08 - 07
    Click on the number of times: 1
    来源:ACS PublicationsThe first ab initio simulation of Magneto-Chiral Dichroism (MChD) for a lanthanide-based complex is reported. The previously experimentally studied [Yb(hfac)3(P–H6bpy)] complex is i...