Crystal Chemistry of NaRE(CO3)2 across Lanthanide Series, Y, and Sc

The date of: 2026-07-08
viewed: 0

来源:ACS Publications

A series of NaRE(CO3)2 compounds (RE = Ce–Lu, Y, Sc) was synthesized under high-pressure and high-temperature and characterized by single-crystal X-ray diffraction and Raman spectroscopy. Combining these data with previously reported results for NaLa(CO3)2 reveals three distinct structure types dictated by the RE3+ species: an orthorhombic phase (Pmc21) for larger REs (La–Nd), a monoclinic phase (P21/c) for smaller ones (Tb–Lu, Y), and a trigonal dolomite-type (CaMg(CO3)2, R3̅) uniquely for Sc. Intermediate rare earths (Sm–Gd) failed to crystallize into NaRE(CO3)2 under our conditions. Structural evolution arises from lanthanide contraction and the rigidity of CO32– units. As the RE3+ radius decreases, RE–O bonds contract, while C–O bonds remain inflexible, causing incomplete bond adjustment and accumulating strain. This strain elevates lattice energy until a phase transition alleviates it, enabling reduced coordination numbers. In the monoclinic phase, positional disorder of Na+ serves as an additional strain-relief mechanism, accommodating a less symmetric coordination environment. The findings elucidate how lanthanide contraction and carbonate rigidity dictate phase transitions and cation disorder, offering critical insights into coordination flexibility in rare-earth chemistry. Moreover, the dolomite-type NaSc(CO3)2 broadens the structural family of rare-earth carbonates and exemplifies heterovalent substitution (Na+ + Sc3+ for Ca2+ + Mg2+).



Hot News / Related to recommend
  • 2026 - 07 - 17
    Click on the number of times: 0
    Hybrid Solvation Model for Analyzing the Binding of Yttrium and Calcium Cations to the Lanmodulin Protein Using the Fragment Molecular Orbital Method 来源:ACS PublicationsA hybrid solvation model combin...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsChemically flexible A2B2O7 oxides are attractive candidates for designing structure-specific functional materials by judicious substitution. However, modulating functionality by sub...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsRational design of Eu2+-activated red phosphors under visible light excitation remains a critical challenge in various fields such as photonics, optoelectronics, and white-light-emi...
  • 2026 - 07 - 15
    Click on the number of times: 0
    来源:ACS PublicationsPolaron formation has emerged as an important mechanism for unconventional luminescence in metal halide semiconductors. Here, we show that incomplete rare-earth-ion doping in the ze...