Leaching of Bastnasite Ore in a Type IV Deep Eutectic Solvent (EG–FeCl3): Taguchi Optimization and Mechanistic Insight by FTIR Evaluation

The date of: 2026-07-02
viewed: 14

来源:ACS Publications

The extraction of rare earth elements (REE) from complex mineral matrices typically relies on hydrometallurgical routes involving strong inorganic acids, which pose significant environmental and operational challenges, including silica gel formation. In this study, a sustainable leaching approach was developed for the recovery of Ce, La, and Nd from calcined bastnasite ore using a nonaqueous type IV deep eutectic solvents (DES) composed of ethylene glycol (EG) and iron(III) chloride (FeCl3). A systematic optimization was conducted using the Taguchi L32 orthogonal array design to evaluate the effects of temperature, solid-to-liquid (S/L) ratio, FeCl3 concentration, leaching time, and stirring speed. Statistical analysis and stepwise regression modeling identified temperature as the most critical parameter governing extraction efficiency, with the regression models exhibiting high predictive accuracy (R2 > 0.87). Molarity and S/L ratio did not exhibit significant effects individually; however, their efficacy became pronounced in conjunction with temperature. The highest total light REE (LREE) extraction efficiency was found to be 62.8% under the conditions of 50 °C, 1 M FeCl3, S/L ratio of 0.05 g/mL, and 16 h. Furthermore, the dissolution mechanism was elucidated using FTIR spectroscopy, which provided direct evidence of an in-situ acidification process. Spectral analysis confirmed that ferric ions coordinate with ethylene glycol to form iron-glycolate complexes, releasing protons that drive the dissolution of REE oxides, with water generated as a stoichiometric byproduct. These findings demonstrate that the EG–FeCl3 system offers a competitive, simplified, and water-free alternative for processing REE ores, 

mitigating the limitations of conventional aqueous methods.


Hot News / Related to recommend
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth hybrid nitrate double perovskites (REHNDPs) have recently emerged as an intriguing subclass of functional materials, combining structural diversity with rich intrinsic op...
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth orthophosphates, REPO4, are highly insulating materials in which localized 4f moments interact through a phosphate framework, providing a model system for weak cooperativ...
  • 2026 - 11 - 06
    Click on the number of times: 4
    来源:ACS PublicationsConventional single-atom alloying (SAA) effect is generally regarded as a design strategy modulating the surface properties of an alloy system between those of its individual elemen...
  • 2026 - 11 - 05
    Click on the number of times: 5
    A system-integrated framework for rare earth element recovery: Source-specific extraction strategies from geological deposits to high-value anthropogenic reservoirs来源:Science DirectRare earth elements...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务