Interstitial Nitrogen Tuning of Magnetocrystalline Anisotropy and High-Frequency Electromagnetic Properties in Nd-Based 3:29-Type Intermetallics

The date of: 2026-06-23
viewed: 10

来源:ACS Publications

The proliferation of 5G/6G communication and millimeter-wave devices has intensified electromagnetic interference, driving demand for thin, broadband microwave absorbers. We report the structure, intrinsic magnetism, and high-frequency electromagnetic response of easy-plane Nd2.7Zr0.3Fe28Ti and its interstitial nitride. Nitrogenation significantly elevates Tc and Ms via the magneto-volume effect (MVE), while the chemical bonding effect (CBE) modulates the crystal field around Nd and markedly enhances the in-plane anisotropy field. The concurrent increase in both anisotropy fields modestly lowers initial permeability, yet the elevated Ms and the concurrent enhancement of both anisotropy fields dominate this trade-off, ultimately raising the natural resonance frequency and extending the operating frequency. Notably, nitrogenation lowers the permittivity through polarized Fe–N and Nd–N bonding, a change intrinsically favorable for impedance matching, offering a route to enhance absorption capability through compositional optimization. This work establishes how the interstitial N effect governs the magnetocrystalline anisotropy and high-frequency electromagnetic response of rare-earth iron intermetallics containing localized 4f electrons, providing a mechanism-driven guideline for designing next-generation soft magnetic absorbers.


Hot News / Related to recommend
  • 2026 - 07 - 17
    Click on the number of times: 0
    Hybrid Solvation Model for Analyzing the Binding of Yttrium and Calcium Cations to the Lanmodulin Protein Using the Fragment Molecular Orbital Method 来源:ACS PublicationsA hybrid solvation model combin...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsChemically flexible A2B2O7 oxides are attractive candidates for designing structure-specific functional materials by judicious substitution. However, modulating functionality by sub...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsRational design of Eu2+-activated red phosphors under visible light excitation remains a critical challenge in various fields such as photonics, optoelectronics, and white-light-emi...
  • 2026 - 07 - 15
    Click on the number of times: 0
    来源:ACS PublicationsPolaron formation has emerged as an important mechanism for unconventional luminescence in metal halide semiconductors. Here, we show that incomplete rare-earth-ion doping in the ze...