Electrochemical Recovery of Rare-Earth Elements from Coal Fly Ash Using Ionic Liquids as both Extractant and Electrolyte

The date of: 2026-05-29
viewed: 7

来源:ACS Publications

Rare-earth elements (REEs) are critical for medical technologies, electronics, and clean energy. Coal fly ash (CFA), a byproduct of coal combustion, offers a promising alternative REE source. However, efficient extraction and separation of REEs from CFA remain challenging due to the complex composition of CFA. This study introduces a sustainable method for REE recovery using a recyclable ionic liquid, betainium bis(trifluoromethylsulfonyl)imide ([Hbet][Tf2N]), which serves both as the extractant from CFA and as the electrolyte in electrodeposition. In the first stage, [Hbet][Tf2N] preferentially extracts REEs from CFA through leaching. In the second stage, the REE-enriched ionic liquid undergoes electrochemical deposition using amperometry techniques, where REEs are reduced and deposited onto the electrode. The deposition experiments were conducted from −0.5 to −2.0 V vs a Pt quasi-reference electrode in a three-electrode setup comprising titanium as the working electrode and platinum as both the reference and counter electrodes. Varying the applied potential enabled potential-dependent preferential REE deposition. At −0.5 V, neodymium (Nd) showed preferential recovery, reaching 25% with a separation factor of 37 over other REEs. In contrast, applying a more negative potential increased overall deposition, yielding ∼50% Nd recovery and 10–20% recovery for the remaining REEs. After recovery, the ionic liquid was regenerated and reused for a subsequent electrochemical recovery cycle. Overall, this study demonstrates a feasible approach for REE recovery from CFA waste, with potential to enhance resource utilization within the REE supply chain.


Hot News / Related to recommend
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe integration of diverse electronic phenomena, such as magnetism and nontrivial topology, into a single low-dimensional system gives rise to unusual quantum effects. Here we combi...
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth elements (REEs: La–Lu, Y, Sc) are critical to modern technology; however, their acquisition, purification, and separation from each other can be challenging, and current ...
  • 2026 - 10 - 08
    Click on the number of times: 0
    来源:ACS PublicationsThe synthesis of alkali-metal-free compounds [LnMe3]n is scrutinized using two distinct protocols. The donor-promoted cleavage of homoleptic tetramethylaluminate complexes Ln(AlMe4)...
  • 2026 - 09 - 30
    Click on the number of times: 0
    来源:ScienceDirectIn the in-situ leaching of ionic rare earth ores, ineffective through-flow induced by ore body heterogeneity and suboptimal rinsing strategies constrain both extraction efficiency and ...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务