Rare-Earth-Driven In Situ Core Evolution: Divergent Assembly of Octamolybdate- and Silverton-Type Templated Silver Nanoclusters

The date of: 2026-05-27
viewed: 0

来源:ACS Publications

Polyoxometalate (POM) anions serve as templates for constructing high-nuclearity silver nanoclusters. Utilizing rare-earth-containing POMs, particularly metastable Silverton-type architectures, remains a synthetic challenge. Herein, a rare-earth-driven in situ core evolution strategy is reported for the construction of a high-nuclearity silver cluster. By introducing dysprosium nitrate, the assembly pathway was redirected from the octamolybdate-templated [Mo8O28@Ag48(CyhS)24(CF3COO)16(CH3CN)4]·5DMF (Mo8@Ag48, CyhS = cyclohexanethiolate) baseline to yield a Silverton-templated [DyMo12O42@Ag54(CyhS)30(CF3COO)6]·9NO3·4CH2Cl2·4DMF (DyMo12@Ag54) cluster. Structural analysis reveals that DyMo12@Ag54 features a pseudoicosahedral Silverton-type [DyMo12O42]9– core. The incorporation of this lanthanide-containing core expands the outer silver shell from 48 to 54 atoms. This “core-swelling” effect and the interaction between the core and shell result in a narrowed optical bandgap, a 3.5-fold increase in photocurrent response, and accelerated photocatalytic degradation kinetics compared to Mo8@Ag48, alongside a red-shift in near-infrared photoluminescence. This work expands the variety of POM templates and demonstrates a strategy for tailoring the properties of silver nanoclusters via inner-template engineering.


Hot News / Related to recommend
  • 2026 - 06 - 09
    Click on the number of times: 0
    来源:ACS PublicationsAtomic structures of a Lu-segregated grain boundary (GB) in α-Al2O3 are identified using hybrid Monte Carlo and molecular dynamics (MCMD) simulations based on a neural-network poten...
  • 2026 - 06 - 08
    Click on the number of times: 0
    来源:ACS PublicationsPrecise control over stereoselective polymerization is crucial for regulating polymer properties. Poly(2-vinylpyridine) (P(2-VP)) represents an important class of polymeric material...
  • 2026 - 06 - 08
    Click on the number of times: 0
    Embedded Hard Base Sites in 1D Covalent Organic Frameworks Enable Selective Photocatalytic Uranium Recovery from Rare Earth Leaching Solution 来源:ACS PublicationsSelective uranium recovery from rare ea...
  • 2026 - 06 - 05
    Click on the number of times: 2
    来源:ACS PublicationsRare-earth-ion-doped disordered crystals are an effective route to spectral broadening. In this study, high-quality Nd:Lu(x)Y(3-x)Ga5O12 composite laser crystals were grown using th...