A Chimeric LBT-GFP Biosensor Exhibits Antithetical Fluorescence Responses to Ca2+ and Dy3+ Binding

The date of: 2026-03-26
viewed: 5

来源:ACS Publications

Rare earth elements (REEs) are critical components in emerging technologies, but their mining and refining processes are often laborious, costly, and environmentally damaging. Developing green and efficient separation methods for REEs is crucial. Biomolecular approaches using lanthanide-binding proteins and peptides show promise for selective REE extraction and separation. In this study, we present the design and characterization of a genetically encoded fluorescence indicator (GEFI) construct that combines a superfolder green fluorescent protein (sfGFP) with a dual lanthanide-binding tag (2×dLBT). The 2×dLBT insert induces conformational changes in sfGFP upon lanthanide binding, modulating the fluorescence intensity. The sfGFP-2×dLBT biosensor exhibited distinct fluorescence responses to different lanthanide ions, with the highest dynamic range observed for heavy REEs like dysprosium (Dy3+). Interestingly, the sensor displayed an antithetical response, where low concentrations of lanthanides initially quenched the fluorescence, but higher concentrations led to a significant fluorescence increase (1.5-fold). The Ca2+ ion on the other hand showed only a dose-dependent quenching of the fluorescence response. Based on these observations, the biphasic response of the biosensor to lanthanides was eliminated by pretreating the sensor with calcium, which further expanded the dynamic range up to 3-fold for Dy3+. The lanthanide-selective and concentration-dependent fluorescence changes of the sfGFP-2×dLBT biosensor demonstrate its potential as a platform for developing specific sensors for various REEs. These sensors could enable rapid and cost-effective determination of REE composition in complex mixtures, facilitating the separation and recovery of critical REEs from electronic waste and other REE-containing sources.


Hot News / Related to recommend
  • 2026 - 04 - 09
    Click on the number of times: 1
    来源:ACS PublicationsCuprous oxide semiconductors have been growing in research interest because of their promising optical and catalytic properties for solar energy conversion. While much recent resear...
  • 2026 - 04 - 08
    Click on the number of times: 2
    来源:ACS PublicationsWe propose to probe the d–f exchange interaction by measuring the response of the itinerant states to an external magnetic field. Two rare-earth monotellurides, TmTe and GdTe, are c...
  • 2026 - 04 - 07
    Click on the number of times: 2
    来源:ACS PublicationsThe electrochemical production of hydrogen peroxide (H2O2) through the two-electron oxygen reduction reaction (2e– ORR) is a sustainable and practical approach that enables efficien...
  • 2026 - 04 - 07
    Click on the number of times: 1
    来源:ACS PublicationsCerium copper oxytelluride (CCOT) and lanthanum copper oxytelluride (LCOT) nanomaterials have been synthesized through a straightforward hydrothermal route to explore their potentia...