SmOBr Quasi-van der Waals Dielectric with High-κ and Ultralow Hysteresis for Two-Dimensional Electronics

The date of: 2026-03-18
viewed: 16

来源:ACS Publications

The integration of two-dimensional (2D) semiconductors into next-generation electronics critically depends on the availability of high-κ dielectrics that combine wide band gaps, strong breakdown fields, and pristine interfaces. Conventional oxides such as HfO2 suffer from interfacial incompatibility with 2D channels, while van der Waals dielectrics like h-BN offer excellent stability but limited capacitance. Here, we report the synthesis of quasi-vdW samarium oxybromide (SmOBr) nanosheets via a molten salt-assisted chemical vapor deposition method, establishing a previously unexplored member of the rare-earth oxyhalide family as a high-performance gate dielectric. SmOBr exhibits a wide band gap (4.63 eV), a high dielectric constant (ε ≈ 13.1), a breakdown field exceeding (EBD) 11.9 MV·cm–1, and ultralow leakage currents (<10–6 μA μm–2), achieving an exceptional balance between dielectric strength and capacitance. When integrated as a top-gate dielectric in MoS2 field-effect transistors, SmOBr enables outstanding device metrics, including subthreshold swings down to 79.5 mV dec–1, Ion/Ioff ratios >107, and ultralow gate hysteresis (∼4.3 mV), with excellent reproducibility and long-term ambient stability. These results position SmOBr as a compelling addition to the quasi-vdW rare-earth dielectric family, with low-power and reliable 2D nanoelectronics.



Hot News / Related to recommend
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsIron (Fe)-rich tailings generated during rare earth element (REE) processing constitute a strategically important secondary resource. However, their utilization is hindered by the r...
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsHigh-entropy rare-earth oxides (HE-REOs) offer a broad compositional space for tuning defect chemistry, lattice distortion, and local atomic environments, yet their controlled synth...
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsSeparation of Rare Earth Elements (REEs) remains an open challenge for their closely related coordination chemistry and hydration. Neodymium (Nd) and yttrium (Y) form an exemplary p...
  • 2026 - 09 - 03
    Click on the number of times: 2
    The Synergistic Impact of Lanthanide-Doped Nickel Iron Sulphides (NiFeSs) Synthesized by a Hydrothermal Method for Effective Water and Urea Electrolysis in Anion Exchange Membranes来源:ACS PublicationsO...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务