Modulation of TSIL-Based Ciprofloxacin Structures with pH for the Selective Extraction of Rare Earth Metals, Uranium, Thorium

The date of: 2026-03-18
viewed: 18

来源:ACS Publications

We report a novel Task-Specific Ionic Liquid (TSIL) derived from ciprofloxacin in combination with CYPHOS·NTf2 that enables tunable selectivity toward the extraction of rare earth metal elements (REEs), thorium, uranium, titanium, and zinc. The highest metal-TSIL affinity was found at pH 6, showing the highest extraction coefficient values for thorium (446), uranium (404), Sc (307), and the remaining REEs, titanium, and zinc (238–71.5; 99; 98). Under highly acidic solutions, however, the TSIL only showed affinity for thorium but not for the remaining species. The metal-cation complexation has been studied by means of NMR spectroscopy and in silico DFT-based optimization of the complexes. The recyclability of the extractive system (up to seven extraction cycles) has also been proved.


Hot News / Related to recommend
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsIron (Fe)-rich tailings generated during rare earth element (REE) processing constitute a strategically important secondary resource. However, their utilization is hindered by the r...
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsHigh-entropy rare-earth oxides (HE-REOs) offer a broad compositional space for tuning defect chemistry, lattice distortion, and local atomic environments, yet their controlled synth...
  • 2026 - 09 - 07
    Click on the number of times: 0
    来源:ACS PublicationsSeparation of Rare Earth Elements (REEs) remains an open challenge for their closely related coordination chemistry and hydration. Neodymium (Nd) and yttrium (Y) form an exemplary p...
  • 2026 - 09 - 03
    Click on the number of times: 2
    The Synergistic Impact of Lanthanide-Doped Nickel Iron Sulphides (NiFeSs) Synthesized by a Hydrothermal Method for Effective Water and Urea Electrolysis in Anion Exchange Membranes来源:ACS PublicationsO...