Enhancing Thermoelectric Performance of n-Type SnSe Polycrystals through Rare-Earth Element Doping and Vacancy Compensation

The date of: 2026-03-09
viewed: 6

来源:ACS Publications

SnSe has attracted considerable interest in thermoelectric research owing to its intrinsically low lattice thermal conductivity and distinctive electronic band structure. However, the development of n-type SnSe remains constrained by the low efficiency of electron doping. In this work, a synergistic strategy involving rare-earth element doping and vacancy compensation is employed to enhance the thermoelectric performance of n-type SnSe polycrystals. Rare-earth elements (La, Ce, Nd, and Pr) are systematically investigated as electron dopants. The results indicate that Pr exhibits the highest doping efficiency in SnSe. In addition, excess Pb is introduced to compensate for intrinsic Sn vacancies, mitigating the vacancy-induced scattering of charge carriers and thereby synergistically optimizing both carrier concentration and carrier mobility. As a result of the significantly enhanced electrical conductivity, the optimized sample Sn0.95Pr0.05Pb0.15Se achieves a maximum ZT value of 1.2 at 773 K. This work presents an effective approach for enhancing the thermoelectric performance of n-type SnSe.



Hot News / Related to recommend
  • 2026 - 04 - 09
    Click on the number of times: 1
    来源:ACS PublicationsCuprous oxide semiconductors have been growing in research interest because of their promising optical and catalytic properties for solar energy conversion. While much recent resear...
  • 2026 - 04 - 08
    Click on the number of times: 2
    来源:ACS PublicationsWe propose to probe the d–f exchange interaction by measuring the response of the itinerant states to an external magnetic field. Two rare-earth monotellurides, TmTe and GdTe, are c...
  • 2026 - 04 - 07
    Click on the number of times: 2
    来源:ACS PublicationsThe electrochemical production of hydrogen peroxide (H2O2) through the two-electron oxygen reduction reaction (2e– ORR) is a sustainable and practical approach that enables efficien...
  • 2026 - 04 - 07
    Click on the number of times: 1
    来源:ACS PublicationsCerium copper oxytelluride (CCOT) and lanthanum copper oxytelluride (LCOT) nanomaterials have been synthesized through a straightforward hydrothermal route to explore their potentia...