An Antipolarity Luminescence Enhancement in DyEu@Gd-MOFs Induced by Isomeric Solvents

The date of: 2026-02-12
viewed: 5

来源:ACS Publications

Highly polar solvents are generally considered to significantly quench the luminous emission of rare-earth doping luminescence materials. In this work, we reported a counterintuitive luminescence phenomenon in Dy/Eu@Gd-MOFs. Their photoluminescence (PL) behaviors in propanol/butanol isomers exhibit trends of emission intensity that inversely correlate with solvent polarity. This phenomenon should not be simplistically ascribed to quenching induced solely by reabsorption, solvent effects, or high-frequency vibrational groups. The structural differences among propanol and butanol isomers result in diversified high-frequency and fingerprint-region vibrational modes. When these vibrations resonate with the critical energy gap, they nonradiative decay in the sensitizer through vibrational coupling, thereby steering energy toward the activator. Time-resolved spectra acquired at different temperatures provide a detailed analysis and evidence for this opinion. These findings give an unconventional interpretation for solvent-induced luminescence quenching in rare-earth luminescence materials, enabling a novel route for modulating their excited states through solvent engineering.



Hot News / Related to recommend
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsSiloxane and aluminol surfaces, ubiquitous in Earth’s system, regulate the adsorption of economically vital elements such as rare earth elements (REEs), yet their atomic-scale react...
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth-doped glasses have great potential in magneto-optical applications due to their high transparency and Verdet constant. However, their synthesis not only requires a high-t...
  • 2026 - 05 - 15
    Click on the number of times: 0
    来源:ACS PublicationsStrong demand for rubber, coupled with limited natural rubber supply, has accelerated the development of synthetic alternatives. Metal-catalyzed polymerization is a key route to hig...
  • 2026 - 05 - 13
    Click on the number of times: 1
    来源:ACS PublicationsIn this study, ZIF-8/HKUST-1 and ZIF-67/HKUST-1 composite materials were fabricated via a stepwise solvent-assisted synthesis route. The materials were characterized by Fourier-tran...