Dense Media Separation for Mineral Carbonation and Enhanced Rare Earth Mineral Recovery

The date of: 2026-02-02
viewed: 15

来源:ACS Publications

Rare earth elements (REEs) play a significant role in a wide range of emerging green energy and defense applications. The increasing demand urges more REE production, thereby necessitating the development of new energy-efficient extraction processing technologies. This study investigated the use of dense media separation (DMS) as a preconcentration technique for sorting REE-bearing ores prior to the conventional beneficiation step. It was demonstrated that DMS can separate most REE-bearing carbonates into the sink fraction, while silicates are separated into the float fraction. Pretreatment effectively reduced the mass and hardness of the materials to be ground. As such, a total grinding energy saving, in some cases, of up to 79.77% and improved REE flotation performance can be achieved compared to the conventional approach. The DMS float fraction enriched with silicates was subjected to mineral carbonation, achieving a carbonation efficiency of approximately 26%. These findings provide compelling evidence that DMS can be used to develop a new energy-efficient REE extraction processing technique while simultaneously offering pathways for CO2 sequestration via the carbonation of gangue minerals.



Hot News / Related to recommend
  • 2026 - 07 - 10
    Click on the number of times: 1
    来源:ACS PublicationsPhotocatalytic activation of C–H bonds in biomass-derived molecules represents a promising strategy for biomass upgrading. However, the efficiency of selective C–H bond activation a...
  • 2026 - 07 - 10
    Click on the number of times: 1
    来源:ACS PublicationsThe escalating global demand for rare earth elements (REE) has highlighted the potential of anthropogenic waste streams as secondary resources. This study characterizes the distribu...
  • 2026 - 07 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe nature of magnetic phase transitions, whether first-order (FOMT) or second-order (SOMT), fundamentally impacts material properties. Doping in alloys can alter this nature, but t...
  • 2026 - 07 - 08
    Click on the number of times: 0
    来源:ACS PublicationsA series of NaRE(CO3)2 compounds (RE = Ce–Lu, Y, Sc) was synthesized under high-pressure and high-temperature and characterized by single-crystal X-ray diffraction and Raman spectro...