High-Entropy Rare Earth Halide Electrolytes with Improved Cycling Stability and Cost Effectiveness

The date of: 2025-08-25
viewed: 34

来源:ACS Publications

Rare earth halide solid state electrolytes (SSEs) have been attracting wide interest recently. However, the high cost of rare earth resources and poor cycling performance in all-solid-state batteries (ASSBs) hinder their practical applications. In this work, two novel high-entropy rare earth halide electrolytes, Li2.6(Y,Ho,Er,Tm,Yb)Cl5.6 (HEE-1) and Li2.6(Y,Ho,Er,Tm,Yb)0.5Zr0.5Cl6.1 (HEE-2), were rationally designed. Both electrolytes use five specially selected rare earth elements to achieve good cost effectiveness. These two electrolytes show high ionic conductivities of 0.52 mS·cm–1 and 1.46 mS·cm–1 at 25 °C, respectively. Lab-scale ASSBs incorporating HEE-1 and HEE-2 exhibit superior high-voltage compatibility and long-cycle stability. The capacity retentions reach 96.2% and 88.1% after 200 cycles, respectively, when charged to 4.5 V (vs Li+/Li) at a rate of 0.3C. Meanwhile, the cell with HEE-2 maintains 91.4% capacity after 1000 cycles between 2.5 and 4.2 V (vs Li+/Li) at a rate of 3C. The high-entropy design enables rare earth halide SSEs with better commercial potentials.

In this work, we adopt a high-entropy strategy to design novel rare earth halide SSEs, aiming to resolve the above concerns. High-entropy materials have been developed rapidly due to their unique structural features, tunable chemical compositions, and superior properties in recent years. A vast number of high-entropy materials, such as alloys, oxides, oxyfluorides, borides, carbides, nitrides, sulfides, and phosphides, have been reported for a wide range of applications including battery materials.




Hot News / Related to recommend
  • 2026 - 04 - 14
    Click on the number of times: 0
    来源:ACS PublicationsAmong rare-earth ions, Dy3+ uniquely enables intrinsic white-light emission and is therefore considered a promising activator for solid-state lighting. However, its parity-forbidden...
  • 2026 - 04 - 14
    Click on the number of times: 0
    来源:ACS PublicationsThe heteroanionic rare-earth germanide oxide Sm26.25Ge22.75O5 was obtained by arc melting. The crystal structure determined by single-crystal X-ray diffraction (space group P4/nmm, ...
  • 2026 - 04 - 13
    Click on the number of times: 0
    来源:ACS PublicationsUnderstanding and modeling energy transfer mechanisms in rare-earth-doped nanomaterials are essential for advancing luminescent technologies used in bioimaging, optical thermometry,...
  • 2026 - 04 - 09
    Click on the number of times: 4
    来源:ACS PublicationsCuprous oxide semiconductors have been growing in research interest because of their promising optical and catalytic properties for solar energy conversion. While much recent resear...