Magnetic and Magnetocaloric Properties of YbVO3 Single Crystals

The date of: 2025-08-07
viewed: 55

Magnetic and Magnetocaloric Properties of YbVO3 Single Crystals Experiments and DFT Calculations


 

来源:ACS Publications

In this paper, we mainly focus on the magnetic and magnetocaloric properties of YbVO3 single crystals grown by the floating-zone method. The crystals present several phase transitions close to 104, 65, and 20 K involving mainly the vanadium sublattice. Particularly, the complex electronic and magnetic structures of YbVO3 result in interesting thermal effects over a wide range of temperatures including a large inverse magnetocaloric effect close to 60 K. In fact, the maximum entropy change is found to be almost 12 J/kg K for a magnetic field change of 0 to 7 T at 64.25 K applied along the c axis and at 65.5 K along the ab plane. More interestingly, the strong magnetocrystalline anisotropy shown by the V3+ sublattice results in a large rotating magnetocaloric effect (RMCE) at relatively high temperatures (60 K). This means that the refrigeration process can be achieved simply by spinning YbVO3 single crystals in constant magnetic fields within the ac or bc planes instead of varying the external magnetic field. Our experimental findings are discussed and analyzed in the framework of Density Functional Theory (DFT) calculations.




Hot News / Related to recommend
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe integration of diverse electronic phenomena, such as magnetism and nontrivial topology, into a single low-dimensional system gives rise to unusual quantum effects. Here we combi...
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth elements (REEs: La–Lu, Y, Sc) are critical to modern technology; however, their acquisition, purification, and separation from each other can be challenging, and current ...
  • 2026 - 10 - 08
    Click on the number of times: 0
    来源:ACS PublicationsThe synthesis of alkali-metal-free compounds [LnMe3]n is scrutinized using two distinct protocols. The donor-promoted cleavage of homoleptic tetramethylaluminate complexes Ln(AlMe4)...
  • 2026 - 09 - 30
    Click on the number of times: 0
    来源:ScienceDirectIn the in-situ leaching of ionic rare earth ores, ineffective through-flow induced by ore body heterogeneity and suboptimal rinsing strategies constrain both extraction efficiency and ...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务