Crystalline Phase Induction Strategy for the Design of Lanthanid

The date of: 2025-05-29
viewed: 29

Crystalline Phase Induction Strategy for the Design of Luminescent Lanthanide Coordination Polymers: Toward Plastic Waste Recycling

 

来源:ACS Publications

Reactions in water between a lanthanide chloride and the disodium salt of tetrachloro-phthalate (tcpa2–) lead to a family of isostructural coordination polymers with the general chemical formula [Ln2(tcpa)3(H2O)4]∞ with Ln = La–Pr (Family 2, F2). The crystal structure was solved based on the La-derivative. It crystallizes in the monoclinic system, space group P21/n (n°14) with the following cell parameters: a = 6.2491(3) Å, b = 17.5805(6) Å, c = 32.1537(14) Å, β = 90.098(2)°, V = 3532.5(3) Å3, and Z = 4. However, this series does not host coordination polymers based on lanthanides that are luminescent in the visible region. These lanthanide ions lead to compounds that crystallize in a previously reported structural family with the general chemical formula [Ln2(tcpa)3(H2O)6]∞ with Ln = Eu–Lu (Family 1, F1). Accordingly, we used a “phase induction strategy” to force Tb3+-, Eu3+-, and Sm3+ -containing molecular alloys to crystallize in F2, and we demonstrate that luminance was optimized when compared with those of F1 despite similar intermetallic energy transfers. This observation was rationalized by theoretical calculations that suggest that the greater rigidity of the crystal structure F2 could be responsible for this notable difference in the luminescence properties.

In this paper, we report the synthesis, the crystal structure, and the luminescent properties of a series of isostructural lanthanide coordination polymers with the general chemical formula [Ln2(tcpa)3(H2O)4]∞ with Ln = La–Pr called Family F2. Because the most luminescent lanthanide ions in the visible domain (Tb3+ and Eu3+) do not lead to this structural type, we use the so-called “phase induction strategy”for preparing heterolanthanide coordination polymers that belong to this structural series but exhibit luminescence in the visible domain. First-principles calculations on [La2(tcpa)3(H2O)y]∞ (y = 4, 6) provide a better understanding of the similarities and differences between the two series.




Hot News / Related to recommend
  • 2026 - 07 - 17
    Click on the number of times: 0
    Hybrid Solvation Model for Analyzing the Binding of Yttrium and Calcium Cations to the Lanmodulin Protein Using the Fragment Molecular Orbital Method 来源:ACS PublicationsA hybrid solvation model combin...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsChemically flexible A2B2O7 oxides are attractive candidates for designing structure-specific functional materials by judicious substitution. However, modulating functionality by sub...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsRational design of Eu2+-activated red phosphors under visible light excitation remains a critical challenge in various fields such as photonics, optoelectronics, and white-light-emi...
  • 2026 - 07 - 15
    Click on the number of times: 0
    来源:ACS PublicationsPolaron formation has emerged as an important mechanism for unconventional luminescence in metal halide semiconductors. Here, we show that incomplete rare-earth-ion doping in the ze...