d0/d10 B'-site doping enables magnetic and magnetocaloric tuning in gadolinium double perovskites

The date of: 2026-11-26
viewed: 0

来源:Communications Materials

In A2BB'O6 double perovskites (DPs) containing 3d and 5d magnetic ions, the magnetic behavior of the B sublattice can be tuned by choosing nonmagnetic isovalent B' cations with d0 or d10 configurations. Here we show that d0/d10 B'-site doping also enables magnetic tuning in 4f7 gadolinium DPs. Substituting Nb5+ (d0) for Sb5+ (d10) in the solid solution Ba2GdNbxSb1-xO6 (0 ≤ x ≤ 1) yields tunable local magnetic correlations that evolve from weak antiferromagnetic (x = 0) through almost suppressed (x = 0.75) to minimal ferromagnetic (x = 1) interactions. B'-site doping modifies the superexchange between nearest-neighbor magnetic spins, allowing controlled suppression of the magnetic ordering temperature. For x = 0.75, where net magnetic interactions are nearly absent, the magnetocaloric effect reaches >99% of the maximum theoretical magnetic entropy for Heisenberg Gd3+ spins at 1.8 K and 9 T, highlighting the potential of this strategy for the rational design of efficient adiabatic demagnetization refrigeration (ADR) materials.


Hot News / Related to recommend
  • 2026 - 11 - 26
    Click on the number of times: 0
    来源:Communications MaterialsIn A2BB'O6 double perovskites (DPs) containing 3d and 5d magnetic ions, the magnetic behavior of the B sublattice can be tuned by choosing nonmagnetic isovalent B' c...
  • 2026 - 11 - 25
    Click on the number of times: 0
    来源:Nature CommunicationsLanthanides serve as essential cofactors in the methanol dehydrogenases of methylotrophic bacteria. While biological function has been characterized for the naturally occurring...
  • 2026 - 11 - 24
    Click on the number of times: 0
    来源:Communications MaterialsConventional polymeric radiation shielding materials suffer from filler aggregation, weak interfacial bonding, and metal leaching. This work presents a chelation immobilizat...
  • 2026 - 11 - 23
    Click on the number of times: 6
    来源:Communications MaterialsSilicon photonics is a solid candidate to address the challenges of emerging communication systems with an increasing number of interconnected devices. However, the properti...