来源:Communications Materials
Conventional polymeric radiation shielding materials suffer from filler aggregation, weak interfacial bonding, and metal leaching. This work presents a chelation immobilization strategy that enables quantitative grafting of high atomic number metals. Gadolinium complexes with a macrocyclic ligand derivative are covalently grafted onto polymer chains through click chemistry, producing stable radiation shielding polymers. Coordination between gadolinium and the ligand induces electron rearrangement, forming multiple hydrogen bonds that act as reversible dynamic crosslinking points. Under mechanical forces, these hydrogen bonds break and rebuild, dissipating energy while enhancing both strength and ductility, overcoming the trade-off between strength and toughness. The polymer exhibits strong attenuation of X and gamma rays and thermal neutrons at low metal loading, remains stable over a wide range of acidity and temperature, and offers good processability and reusability. The study resolves the conflict between high shielding efficiency and lightweight flexibility, offering a route toward next-generation transparent, lightweight, and wearable nuclear radiation shielding materials.