Securing critical rare-earth supply through end-of-life NdFeB magnets recycling via molten salt electrolysis with consumable Mg-cathode

The date of: 2026-11-12
viewed: 0

来源:Nature Communications

Recycling end-of-life (EoL) NdFeB magnets is critical for securing supply of rare-earth element neodymium in the low-carbon transition. We develop a molten salt electrolysis recycling approach using EoL NdFeB magnet anodes and a consumable solid magnesium cathode, operating at 548–650 °C and 0.75–3 A·cm⁻² cathodic current density. Selective neodymium dissolution and in situ formation of a liquid Mg–(12.0–15.1 mol%) Nd alloy with average current efficiency of 98.4% are achieved. With high recycling efficiency and continuous operation, this approach overcomes neodymium collection and scalability barriers of conventional chloride electrolysis. Life-cycle assessment shows that the proposed process lowers climate change impacts to 17.36–18.18 kg CO₂ eq.·kg⁻¹ Nd, approximately 15% of that of primary production. Techno-economic analysis shows that neodymium metal production costs fall to 90.0 USD·kg⁻¹ Nd at the 3000 A scale scenario, which is approximately one-third lower than the sales price of Nd metal. Such approach demonstrates significant potential for industrial-scale application and facilitates the integration of neodymium recycling into circular economy strategies.


Hot News / Related to recommend
  • 2026 - 11 - 13
    Click on the number of times: 0
    来源:Nature CommunicationsQuantifying three-dimensional (3D) orientation is critical for understanding self-assembly and collective behavior in soft matter and biological systems. Moreover, orientationa...
  • 2026 - 11 - 12
    Click on the number of times: 0
    来源:Nature CommunicationsRecycling end-of-life (EoL) NdFeB magnets is critical for securing supply of rare-earth element neodymium in the low-carbon transition. We develop a molten salt electrolysis re...
  • 2026 - 11 - 11
    Click on the number of times: 3
    来源:Science DirectZrB2-SiC ceramic composites are susceptible to severe oxidation corrosion at 1700 ℃ in oxidizing atmospheres, owing to rapid B2O3 volatilization, ZrO2-transformation-induced cracking,...
  • 2026 - 11 - 11
    Click on the number of times: 2
    Process intensification of low-concentration magnesium sulfate leaching of ion-adsorption rare earth ores by pulsed microwave-assisted gradient injection来源:Science DirectRare earth elements (REEs), pa...