Inorganic Phosphate-Mediated Efficient Fabrication of Phosphate Ester-Functionalized Stationary Phases for Full-Series Rare Earth Element Separation

The date of: 2026-10-26
viewed: 1

来源:ACS Publications 

Rare earth elements (REEs) are irreplaceable in advanced new materials and high-end manufacturing industries. However, their nearly identical physicochemical properties, coupled with the associated diverse impurities, render the full separation of REEs a long-standing and formidable challenge in analytical separation science. In this work, a novel phosphate ester-functionalized cation-exchange stationary phase (Sil-PCX) was successfully developed for the first time via a simple inorganic phosphate-mediated synthesis. Benefiting from the moderate ion-exchange characteristics of phosphate ester groups, the proposed stationary phase accomplished the complete separation of the entire series of REEs within 55 min and afforded a high resolution of 2.6 for the hard-to-separate Dy/Y pair. Stability tests revealed that the relative standard deviation (RSD) of retention times for all REEs was below 0.23% following ten consecutive injections, which verified the excellent reproducibility and operational stability of the developed stationary phase. Moreover, the sub-2 μm Sil-PCX enables ultrafast separation of REEs within 10 min, providing a robust technical foundation for the precise quantitative analysis and detection of all REEs. Notably, the stationary phase demonstrated remarkable separation capability for REEs and radioactive nuclide impurities, enabling efficient removal of radioactive contaminants (U and Th) from REE matrices. Furthermore, density functional theory (DFT) calculations have elucidated the mechanism of chromatographic separation of REEs on Sil-PCX. Overall, the phosphate ester-based column exhibited superior separation performance and excellent stability, meeting the requirements of both analytical determination and large-scale preparation of high-purity REEs.



Hot News / Related to recommend
  • 2026 - 10 - 27
    Click on the number of times: 0
    来源:ACS PublicationsRare earth elements are critical to decarbonization, advanced electronics, and defense applications. Traditional hydrometallurgical recovery using liquid–liquid solvent extraction (...
  • 2026 - 10 - 26
    Click on the number of times: 1
    来源:ACS Publications Rare earth elements (REEs) are irreplaceable in advanced new materials and high-end manufacturing industries. However, their nearly identical physicochemical properties, c...
  • 2026 - 10 - 26
    Click on the number of times: 1
    来源:ACS PublicationsThe efficient recovery of rare-earth elements (REEs) from wastewater is crucial for resource utilization and environmental protection. Developing adsorbents with green fabrication p...
  • 2026 - 10 - 23
    Click on the number of times: 2
    来源:Science DirectThe use of rare earth compounds as ceramic coatings to protect engine turbines blades from chemical degradation has been widely studied in the last two decades. After interaction with...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务