Interstitial Rare-Earth Doping of FAPbI3 Perovskite Nanocrystals under Mild Ambient Conditions

The date of: 2026-10-14
viewed: 0

来源:ACS Publications

The rare-earth (RE) metal doping strategies have been investigated for many applications in perovskite materials. However, prior approaches to synthesizing RE-doped perovskite nanocrystals (PNCs) have predominantly required harsh synthesis conditions, including an inert gas atmosphere and high temperatures. Here, we present a doping strategy using four RE ions (La3+, Nd3+, Gd3+, and Er3+) doped into FAPbI3 PNCs under mild conditions (50 °C) in an ambient atmosphere. Density functional theory calculations were performed to rationalize the RE incorporation by evaluating the formation energy of possible dopant configurations within the FAPbI3 lattice. The results demonstrated that RE ions were successfully introduced into interstitial sites in the FAPbI3 lattice under mild conditions. RE-doped FAPbI3 PNCs were demonstrated to preserve the structure of α-FAPbI3 PNCs, while improving the optical properties in colloidal and thin-film samples, delivering an enhanced power conversion efficiency of 18.65% in photovoltaic performance together with improved stability relative to pristine PNCs.


Hot News / Related to recommend
  • 2026 - 10 - 22
    Click on the number of times: 0
    Mechanisms of rare earth element and aluminum leaching with magnesium sulfate based on coupled seepage–chemical–diffusion simulations in microporous networks来源:Science DirectIn situ leaching of ionic ...
  • 2026 - 10 - 22
    Click on the number of times: 0
    来源:Science DirectRare-earth mono-nitrides (REN) are important rare-earth compounds whose structural stability and electronic structure are strongly influenced by localized 4f states. In this work, a f...
  • 2026 - 10 - 21
    Click on the number of times: 0
    来源: Science DirectThe reason for the higher extraction rate of light rare earth elements (LREY) than that of heavy rare earth elements (HREY) during the extraction of rare earth elements (REY) from co...
  • 2026 - 10 - 20
    Click on the number of times: 0
    来源:ACS Publications High-quality single crystals of refractory oxides are essential for fundamental investigations and advanced functional characterization, yet their preparation is frequentl...