Dual Electronic and Interfacial Microenvironment Modulation on Rare-Earth Doped Ternary Pt Alloys Toward Alkaline Hydrogen Oxidation

The date of: 2026-09-24
viewed: 9

来源:ACS Publications

Alkaline hydrogen oxidation reaction (HOR) is the bottleneck restricting the performance of anion-exchange membrane fuel cells (AEMFCs), originating from sluggish Volmer kinetics induced by mismatched adsorption of H* and OH intermediates on commercial Pt/C catalysts, accompanied by high Pt cost, poor durability and inferior CO tolerance. Herein, Pr-doped PtMo ternary nanoparticles anchored on XC-72 carbon (PtMoPr/C) are fabricated via a facile wet chemical reduction strategy, where trace Pr dopant regulates electronic configuration and lattice strain of PtMo via unique 4f-5d orbital hybridization. Operando characterizations and DFT calculations verify that Pr induces downshifted Pt d-band center to weaken excessive Pt–H binding, provides abundant OH adsorption sites to accelerate Volmer step. Electronic modulation by Pr also increases the interfacial water and enhances the connectivity of hydrogen-bond networks within the electric double layers, synergistically boosting alkaline HOR performance. Electrochemical measurements demonstrate that the optimized PtMoPr/C delivers a mass activity of 2656.9 mA mgpt–1 at 50 mV vs RHE in 0.1 M KOH, 16-fold higher than that of benchmark Pt/C, together with outstanding anti-CO poisoning capability when exposed to CO-containing H2 feedstock. This work clarifies rare-earth Pr’s multifunctional effects and proposes an orbital modulation route to develop low-Pt HOR catalysts for practical AEMFC.


Hot News / Related to recommend
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth hybrid nitrate double perovskites (REHNDPs) have recently emerged as an intriguing subclass of functional materials, combining structural diversity with rich intrinsic op...
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth orthophosphates, REPO4, are highly insulating materials in which localized 4f moments interact through a phosphate framework, providing a model system for weak cooperativ...
  • 2026 - 11 - 06
    Click on the number of times: 4
    来源:ACS PublicationsConventional single-atom alloying (SAA) effect is generally regarded as a design strategy modulating the surface properties of an alloy system between those of its individual elemen...
  • 2026 - 11 - 05
    Click on the number of times: 5
    A system-integrated framework for rare earth element recovery: Source-specific extraction strategies from geological deposits to high-value anthropogenic reservoirs来源:Science DirectRare earth elements...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务