Exploratory Evaluation of Er/Y-Modified RuO2 for Acidic Oxygen Evolution

The date of: 2026-08-19
viewed: 18

来源:ACS Publications

The intrinsic instability of ruthenium dioxide (RuO2) under acidic oxygen evolution reaction (OER) conditions remains a critical challenge for the development of durable OER electrocatalysts. Here, we present an exploratory comparative half-cell investigation of one nominal Er/Y-modified RuO2 composition. Under the specified conditions (0.1 M HClO4, room temperature, three-electrode configuration), Er0.1Y0.1Ru0.8O2 required 226 mV to reach 10 mA cm–2, compared with 257 mV for identically prepared h-RuO2. During an 80,000 s chronopotentiometry test, the modified sample showed lower Ru leaching than h-RuO2 (117 versus 281 μg L–1). Fresh-state XRD, HRTEM, XPS, EIS, and DFT-PDOS identify structural and electronic differences that are consistent with a qualitative working model of Er/Y modification. The current data do not establish individual Er/Y contributions, an Er/Y-ratio-performance relationship, an OER pathway, or PEMWE/MEA performance. Systematic composition-controlled, operando, and device-level measurements are required to test these questions.


Hot News / Related to recommend
  • 2026 - 11 - 20
    Click on the number of times: 2
    来源:Nature CommunicationsEfficient 1.54 µm electroluminescence from erbium ions has long been hindered by their intrinsically small absorption cross-section and low excitation efficiency in conven...
  • 2026 - 11 - 19
    Click on the number of times: 2
    来源:Nature CommunicationsDry reforming of methane (DRM) with carbon dioxide produces CO-rich syngas for methanol and Fischer–Tropsch fuel synthesis, but carbon deposition deactivates catalysts and limi...
  • 2026 - 11 - 18
    Click on the number of times: 2
    来源:Nature CommunicationsSpatial-light computing requires rewritable, multilevel and persistent optical weights, but many implementations rely on volatile modulators or static power. Here we report a C...
  • 2026 - 11 - 17
    Click on the number of times: 6
    来源:Nature CommunicationsLanthanide-doped upconversion nanoparticles exhibit multicolor emission through discrete, narrowband transitions, enabling applications in bioimaging, lasers, and displays. How...