Electronic Structure Engineering of Ni2P via Er/Fe Co-Doping for Enhanced Oxygen Evolution Reaction Electrocatalysis

The date of: 2026-05-07
viewed: 18

来源:ACS Publications


The oxygen evolution reaction (OER) is a critical yet kinetically sluggish process in water electrolysis for hydrogen generation, owing to its multistep, four-electron transfer. This necessitates the development of efficient catalysts to accelerate the reaction. Herein, Er/Fe-codoped Ni2P supported on nickel foam (Er/Fe−Ni2P/NF) was fabricated via an electrodeposition−phosphorization approach to explore the Er/Fe synergistic effects on OER dynamics. The results demonstrate that Er/Fe codoping effectively modulates the electronic structure of the catalyst and accelerates charge transfer kinetics. The optimized catalyst exhibits superior performance requiring only 208 ± 1 mV to achieve 10 mA cm−2 with a low Tafel slope of 33.66 mV dec−1, along with durability over 50 h of continuous testing. In situ Raman and infrared spectroscopic investigations demonstrate that Er/Fe codoping not only reduces the formation potential of NiOOH but also accelerates its formation kinetics. Density functional theory (DFT) calculations further elucidate that doping alters the *O adsorption configuration, while Er/Fe codoping further optimizes the reaction pathway, reducing the energy barrier and thus achieving exceptional OER catalytic performance.



Hot News / Related to recommend
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth hybrid nitrate double perovskites (REHNDPs) have recently emerged as an intriguing subclass of functional materials, combining structural diversity with rich intrinsic op...
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth orthophosphates, REPO4, are highly insulating materials in which localized 4f moments interact through a phosphate framework, providing a model system for weak cooperativ...
  • 2026 - 11 - 06
    Click on the number of times: 4
    来源:ACS PublicationsConventional single-atom alloying (SAA) effect is generally regarded as a design strategy modulating the surface properties of an alloy system between those of its individual elemen...
  • 2026 - 11 - 05
    Click on the number of times: 5
    A system-integrated framework for rare earth element recovery: Source-specific extraction strategies from geological deposits to high-value anthropogenic reservoirs来源:Science DirectRare earth elements...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务