Influence of Nd(II) and Nd(III) Ions on the Speciation and Kinetic Dynamics of Radiolytic Transients in Molten LiCl-KCl

The date of: 2026-01-22
viewed: 21

来源:ACS Publications

In the pyrochemical reprocessing of used nuclear fuel, understanding the effects of ionizing radiation on the chemical behavior of fission products in molten chloride eutectic salt is crucial. This study investigates the impact of radiation on the chemical and kinetic speciation of Nd ions in molten LiCl-KCl eutectic, which are challenging to separate due to their multivalent oxidation states and comproportionation reactions. Electron pulse radiolysis techniques were used to determine transient absorption spectra, chemical kinetics, and activation parameters for the reaction of Nd ions with the primary products of molten LiCl-KCl eutectic radiolysis: the solvated electron (eS–) and dichlorine radical anion (Cl2•–). Initially, Nd(III) reacted rapidly with eS–, forming Nd(II) with a second-order rate coefficient of k = (4.54 ± 0.07) × 1010 M–1 s–1 at 673 K. The resulting Nd(II) ions then reacted slowly with Cl2•–, regenerating Nd(III) with an estimated rate of k = (1.72 ± 0.04) × 1010 M–1 s–1 at 673 K. Additionally, the comproportionation reaction of Nd(III) and Nd(s) to form Nd(II) was monitored chemically and electrochemically. This work suggests that the comproportionation reaction of Nd(III) with Nd(s) to form Nd(II) is unstable in molten LiCl-KCl eutectic.


Hot News / Related to recommend
  • 2026 - 10 - 30
    Click on the number of times: 0
    来源:Science DirectFluoride in ionic rare earth ore leachate readily induces three-phase emulsification during rare earth solvent-extraction process, severely worsening separation efficiency and product...
  • 2026 - 10 - 30
    Click on the number of times: 1
    来源:Science DirectProlonged MgSO4 in-situ leaching (ISL) of ion-adsorption rare earth element deposits may alter rare earth elements (REEs) vertical distribution, fractionation, and speciation, but fie...
  • 2026 - 10 - 29
    Click on the number of times: 0
    来源:ACS PublicationsTo ensure supply chain security, highly selective recovery of rare-earth elements (REEs) from industrial solid wastes is essential. In this study, UiO-66-NH2 was functionalized with...
  • 2026 - 10 - 28
    Click on the number of times: 0
    来源:ACS PublicationsRare earth elements, characterized by their partially filled 4f orbitals and exceptional electron transfer capabilities, play an irreplaceable regulatory role in both acid-base and ...