Unveiling the Role of Ce 4f Orbitals in Modulating MnO2 Oxygen Evolution Reaction Performance

The date of: 2025-12-16
viewed: 43

来源:ACS Publications

Due to its strong acid and oxidation resistance, rutile β-MnO2 is considered to be a highly promising acidic nonprecious metal OER catalyst. However, the direct electron supply located in the Mn–O energy band below the Fermi energy level (Ef) causes instability of the Mn–O bond, making the long-term activity and stability of β-MnO2 poor. However, in this paper, introducing Ce 4f orbitals to construct a simultaneous Mn–O electronic configuration improved by the electronic buffer band through electronic coupling is proposed, thus enhancing the OER activity and stability. The combination of electronic structure characterization (XASF, XPS, in situ Raman, etc.) and theoretical calculation analysis reveals that the constructed Ce(f)–O(p)–Mn(d) orbital coupling electronic structure enhances the Mn–O covalent bonding and improves the adsorption capacity of O*, which enhances the OER activity of β-MnO2. Moreover, Ce 4f acts as a buffer band to stabilize the Mn site and avoid the excessive oxidation of Mn, thus enhancing the stability of β-MnO2.



Hot News / Related to recommend
  • 2026 - 09 - 03
    Click on the number of times: 2
    The Synergistic Impact of Lanthanide-Doped Nickel Iron Sulphides (NiFeSs) Synthesized by a Hydrothermal Method for Effective Water and Urea Electrolysis in Anion Exchange Membranes来源:ACS PublicationsO...
  • 2026 - 09 - 03
    Click on the number of times: 2
    来源:ACS PublicationsMixed valency in compounds containing rare-earth elements can lead to intriguing properties, such as complex magnetism, unique charge transport, and superconductivity. Zintl A14MPn1...
  • 2026 - 09 - 02
    Click on the number of times: 2
    来源:ACS PublicationsEfficient and green separation of rare earth elements (REE) remains a critical challenge, with conventional solvent extraction relying heavily on toxic organic solvents. Herein, thr...
  • 2026 - 09 - 01
    Click on the number of times: 1
    来源:ACS PublicationsRare-earth activation in oxide thin films is often optimized empirically, although excitation-dependent upconversion (UC) is ultimately constrained by the near-surface energetic lan...