Recovering in-demand metals for new electronics

The date of: 2024-11-21
viewed: 26
Recovering in-demand metals for new electronics—researchers find industrial-strength adsorbents soak up lanthanum


                
source: Canadian Light Source
Nearly all technology today—from cellphones to computers to MRI scanners—contains rare earth elements (REEs). The global market for REEs is predicted to reach $6.2 billion (USD) this year and $16.1 billion (USD) by 2034.
High concentrations of one particular REE—lanthanum—are often found in mine tailings. Runoff from this waste can make its way into nearby bodies of water where it poses a risk to human health and the environment. As a result, researchers are on the hunt for ways to recover the material.
Michael Chan, working under the supervision of Dr. Huu Doan in the Department of Chemical Engineering at Toronto Metropolitan University (TMU), recently discovered that industrial-strength chemical adsorbents can be used to "soak up" lanthanum from that mine waste. The research is published in the journal Inorganics.
"These 'fancy sponges' are about the size of a grain of salt," says Chan, who is completing his Masters degree at TMU. Working in a lab, Chan and his colleagues found that the metal ions present in a sample of contaminated water trade places with the hydrogen ions present on the surface of adsorbent.
When they filtered the adsorbent out of the water, they were left with cleaner water and recovered lanthanum that could be reformed and reused in new electronics.
The team used a scanning electron microscope at TMU to better understand the ion exchange process, then used the Canadian Light Source at the University of Saskatchewan to get even more detailed images and to confirm their findings.
"The exciting part about these findings is that this is something that we can do now, today," says Chan. "We can use what we have. We can really give it a shot and apply it to real-life situations and industry."
Chan and his team collaborated with Dr. Trong Dang-Vu from SNF Canada, a company specializing in water treatment solutions.
"They were able to guide us in terms of what industry is looking for," says Chan. "They also provided us with tailings samples from mines, so in further research we'll see if we can use those samples and see just how effective this approach really is."



Hot News / Related to recommend
  • 2026 - 10 - 22
    Click on the number of times: 0
    Mechanisms of rare earth element and aluminum leaching with magnesium sulfate based on coupled seepage–chemical–diffusion simulations in microporous networks来源:Science DirectIn situ leaching of ionic ...
  • 2026 - 10 - 22
    Click on the number of times: 0
    来源:Science DirectRare-earth mono-nitrides (REN) are important rare-earth compounds whose structural stability and electronic structure are strongly influenced by localized 4f states. In this work, a f...
  • 2026 - 10 - 21
    Click on the number of times: 0
    来源: Science DirectThe reason for the higher extraction rate of light rare earth elements (LREY) than that of heavy rare earth elements (HREY) during the extraction of rare earth elements (REY) from co...
  • 2026 - 10 - 20
    Click on the number of times: 0
    来源:ACS Publications High-quality single crystals of refractory oxides are essential for fundamental investigations and advanced functional characterization, yet their preparation is frequentl...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务