Rapid and precise large area mapping of rare-earth doping homogeneity in luminescent materials
The date of:
2024-11-19
viewed:
40
source:Communications Materials
Doping of luminescent materials by rare-earth ions is common practice to achieve desired emission properties for a large variety of applications. As several rare-earths ions are frequently combined, it is subsequently difficult to effectively detect and control their homogeneous distribution within the host material. Here, we present a simple, rapid, large scale and precise method of rare-earth mapping using a commercial UV-Vis scanner. We discuss the influence of rare-earth distribution on the physical, optical and luminescent properties with no observable qualitative effect on photoluminescent properties and optical anisotropy. On the contrary, rare-earth-rich areas exhibit significantly higher values of refractive index and optical absorption, which allowed for their identification by the commercial scanner device. The presented method thus provides fast and accurate information about the rare-earth distribution in the material volume with high resolution (≈2.7 µm) and low limit of concentration difference detection (≈0.014 at.%) compared to other techniques, which makes it a promising candidate for high throughput measurements.
Hot News
/
Related to recommend
2026
-
10
-
27
Click on the number of times:
0
来源:ACS PublicationsRare earth elements are critical to decarbonization, advanced electronics, and defense applications. Traditional hydrometallurgical recovery using liquid–liquid solvent extraction (...
2026
-
10
-
26
Click on the number of times:
1
来源:ACS Publications Rare earth elements (REEs) are irreplaceable in advanced new materials and high-end manufacturing industries. However, their nearly identical physicochemical properties, c...
2026
-
10
-
26
Click on the number of times:
3
来源:ACS PublicationsThe efficient recovery of rare-earth elements (REEs) from wastewater is crucial for resource utilization and environmental protection. Developing adsorbents with green fabrication p...
2026
-
10
-
23
Click on the number of times:
2
来源:Science DirectThe use of rare earth compounds as ceramic coatings to protect engine turbines blades from chemical degradation has been widely studied in the last two decades. After interaction with...