‘Exceptional’ rare earth grades at Caldas

The date of: 2024-10-25
viewed: 25
source:Australian Resources & Investment


Axel REE has intersected “exceptional concentrations” of rare earth elements as part of an auger drilling campaign at its Caldas project, part of the Poços de Caldas Alkaline Complex in Minas Gerais, Brazil.
Results from drill hole CAL-AUG-001 returned 11m at 3273 parts per million (ppm) total rare earth oxide (TREO), including 1m at 7099ppm TREO and 3m at 5609ppm TREO, ending in high-grade mineralisation and indicating potential depth continuity.
Other impressive results included CAL-AUG-003, which reported 20m at 3082ppm TREO, including 1m at 6536ppm TREO.
“We are extremely pleased with our initial auger drill assay results showing high-grade TREO from our Caldas project within the Poços de Caldas Alkaline Complex,” Axel managing director Fernando Tallarico said.
“This first batch demonstrates the significant surface mineralisation of our project area and underscores the discovery potential of the project area.”
One of the key findings is the significant concentration of high-value magnet rare earth oxides (MREO), which accounted for up to 36 per cent of the TREO in some samples, highlighting the potential of the project to feed renewable energy technologies.
“The most exciting aspect of these initial results is that all holes returned increasingly high-grade TREO mineralisation at end of hole, which, similar to that of our peers at the Poços de Caldas, demonstrates the significant potential for a discovery zone at depth,” Tallarico said.
“In addition, this is just the first batch as we expect to progressively receive auger results from our Caldas project as well as diamond drill results at our Caladão project in the Lithium Valley.”
At the Caladão project, Axel has completed 77 drill holes with additional samples sent for analysis.
Subscribe to Australian Resources & Investment and receive the latest news on commodity prices, resource developments, executive movements and more.



Hot News / Related to recommend
  • 2026 - 10 - 22
    Click on the number of times: 0
    Mechanisms of rare earth element and aluminum leaching with magnesium sulfate based on coupled seepage–chemical–diffusion simulations in microporous networks来源:Science DirectIn situ leaching of ionic ...
  • 2026 - 10 - 22
    Click on the number of times: 0
    来源:Science DirectRare-earth mono-nitrides (REN) are important rare-earth compounds whose structural stability and electronic structure are strongly influenced by localized 4f states. In this work, a f...
  • 2026 - 10 - 21
    Click on the number of times: 0
    来源: Science DirectThe reason for the higher extraction rate of light rare earth elements (LREY) than that of heavy rare earth elements (HREY) during the extraction of rare earth elements (REY) from co...
  • 2026 - 10 - 20
    Click on the number of times: 0
    来源:ACS Publications High-quality single crystals of refractory oxides are essential for fundamental investigations and advanced functional characterization, yet their preparation is frequentl...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务