High concentrations of rare earths found in Utah, Colorado coal mines

The date of: 2024-05-27
viewed: 40
source:mining


Research led by the University of Utah has documented elevated concentrations of rare earth elements, or REEs, in active mines rimming the Uinta coal belt of Colorado and Utah.
The work, published in the journal Frontiers in Earth Science, explains that these mines could see a secondary resource stream in the form of metals used in renewable energy and numerous other high-tech applications.
“The model is if you’re already moving rock, could you move a little more rock for resources towards energy transition?,” study co-author Lauren Birgenheier said in a media statement. “In those areas, we’re finding that the rare earth elements are concentrated in fine-grain shale units, the muddy shales that are above and below the coal seams.”
This research was conducted in partnership with the Utah Geological Survey and Colorado Geological Survey as part of the Carbon Ore, Rare Earth and Critical Minerals project, or CORE-CM.
While these metals are crucial for US manufacturing, especially in high-end technologies, they are largely sourced from overseas.
“When we talk about them as ‘critical minerals,’ a lot of the criticality is related to the supply chain and the processing,” Michael Free, who also authored the paper, said. “This project is designed around looking at some alternative unconventional domestic sources for these materials.”
Hard, abundant data
The association between coal and REE deposits has been well documented elsewhere, but little data had been previously gathered or analyzed in Utah and Colorado’s coal fields.
“The goal of this phase-one project was to collect additional data to try and understand whether this was something worth pursuing in the West,” said study co-author Michael Vanden Berg, energy and minerals program manager at the Utah Geological Survey. “Is there rare earth element enrichment in these rocks that could provide some kind of byproduct or value added to the coal mining industry?”
The researchers analyzed 3,500 samples from 10 mines, four mine waste piles, seven stratigraphically complete cores, and even some coal ash piles near power plants.
“The coal itself is not enriched in rare earth elements,” Vanden Berg said. “There’s not going to be a byproduct from mining the coal, but for a company mining the coal seam, could they take a couple of feet off the floor at the same time? Could they take a couple of feet off the ceiling? Could there be potential there? That’s the direction that the data led us.”
The team deployed two different methods to record levels of rare earths, expressed in parts per million, or ppm, in the samples. One was a hand-held device for quick readings in the field, the other used Inductively Coupled Plasma-Mass Spectrometry, or ICP-MS, in an on-campus lab.
“We’re mostly using this portable X-ray fluorescence device, which is an analysis gun that we hold to the rock for two minutes, and it only gives us five or six of the 17 rare earth elements,” Birgenheier said. If samples showed concentrations higher than 200 ppm, they ran a more complete analysis using the more costly mass spectrometry equipment.
The Department of Energy has set 300 ppm as the minimum concentration for rare earth mining to be potentially economically viable. However, for the study, the researchers deemed concentrations greater than 200 ppm to be considered “REE enriched.”
The analysis found the highest prevalence of such concentrations in coal-adjacent formations of siltstone and shale, while sandstone and the coal itself were mostly devoid of rare earths.
So far, the team has analyzed 11,000 samples. Next steps include determining how much rare earth ore is present, likely to be done with colleagues at the University of Wyoming and New Mexico Institute of Mining and Technology.



Hot News / Related to recommend
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth hybrid nitrate double perovskites (REHNDPs) have recently emerged as an intriguing subclass of functional materials, combining structural diversity with rich intrinsic op...
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth orthophosphates, REPO4, are highly insulating materials in which localized 4f moments interact through a phosphate framework, providing a model system for weak cooperativ...
  • 2026 - 11 - 06
    Click on the number of times: 4
    来源:ACS PublicationsConventional single-atom alloying (SAA) effect is generally regarded as a design strategy modulating the surface properties of an alloy system between those of its individual elemen...
  • 2026 - 11 - 05
    Click on the number of times: 5
    A system-integrated framework for rare earth element recovery: Source-specific extraction strategies from geological deposits to high-value anthropogenic reservoirs来源:Science DirectRare earth elements...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务