‘Significant breakthrough’: This new sea-salt battery has 4 times the capacity of lithium

The date of: 2022-12-14
viewed: 27

source:euronews


Your electronics could soon be powered by an ultra cheap sea salt battery.

Researchers have built a new cheap battery with four times the energy storage capacity of lithium.

Constructed from sodium-sulphur - a type of molten salt that can be processed from sea water - the battery is low-cost and more environmentally friendly than existing options. 

It could be a ‘breakthrough’ for renewable energy, according to lead researcher Dr Shenlong Zhao, from the University of Sydney.

“Our sodium battery has the potential to dramatically reduce costs while providing four times as much storage capacity [as Lithium],” he said.

“This is a significant breakthrough for renewable energy development which, although reduces costs in the long term, has had several financial barriers to entry.”

In pictures: South America's 'lithium fields' reveal the dark side of our electric future

France's massive new lithium mine could supply 700,000 electric car batteries a year

Why do batteries matter to renewable energy?

As the climate heats up, there is an urgent need to switch to renewable energy sources like wind and solar. But renewables are not always as consistent as other sources meaning batteries are needed to store this electricity for later use.

Many batteries are built with rare earth metals like lithium, graphite, and cobalt.

To achieve climate neutrality, the EU will require 18 times more lithium than it currently uses by 2030 and almost 60 times more by 2050.

European Commission President Ursula von der Leyen said in September that 'lithium and rare earths will soon be more important than oil and gas.'

But these metals come at a cost. Lithium extraction can result in water shortages, biodiversity loss, damage to ecosystem functions and soil degradation.

When the metal is produced using evaporation ponds, for example, it takes approximately 2.2 million litres to produce one metric tonne.

It’s also financially costly to mine at scale. This is where the sea salt battery could provide an alternative.

Good eggs: Eggs can be used to filter microplastics and salt out of water, research finds

Two e-cigarettes are thrown away every second in the UK. What damage do they do?

What are molten salt batteries and are they scalable?

Molten salt batteries aren’t a new concept. They’ve been around for 50 years, but they’ve been an ‘inferior alternative’ with a short energy life cycle.

But this new battery is different. Scientists altered the electrodes to improve the reactivity of the sulphur - a key element determining storage capacity.

Canva

Lithium ion batteries are important to the electric car revolution - but they can be environmentally damaging.Canva

The resulting product showed “super-high capacity and ultra-long life at room temperature,” the University of Sydney researchers advise.

Because sea salt is everywhere, it could provide a scalable alternative to lithium ion batteries.

“When the sun isn’t shining and the breeze isn’t blowing, we need high-quality storage solutions that don’t cost the Earth and are easily accessible on a local or regional level,” Dr Zhao said.

“Storage solutions that are manufactured using plentiful resources like sodium – which can be processed from sea water – also have the potential to guarantee greater energy security more broadly and allow more countries to join the shift towards decarbonisation.”

The researchers now plan to improve and commercialise the new cells.



Hot News / Related to recommend
  • 2026 - 09 - 03
    Click on the number of times: 2
    The Synergistic Impact of Lanthanide-Doped Nickel Iron Sulphides (NiFeSs) Synthesized by a Hydrothermal Method for Effective Water and Urea Electrolysis in Anion Exchange Membranes来源:ACS PublicationsO...
  • 2026 - 09 - 03
    Click on the number of times: 2
    来源:ACS PublicationsMixed valency in compounds containing rare-earth elements can lead to intriguing properties, such as complex magnetism, unique charge transport, and superconductivity. Zintl A14MPn1...
  • 2026 - 09 - 02
    Click on the number of times: 2
    来源:ACS PublicationsEfficient and green separation of rare earth elements (REE) remains a critical challenge, with conventional solvent extraction relying heavily on toxic organic solvents. Herein, thr...
  • 2026 - 09 - 01
    Click on the number of times: 1
    来源:ACS PublicationsRare-earth activation in oxide thin films is often optimized empirically, although excitation-dependent upconversion (UC) is ultimately constrained by the near-surface energetic lan...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务