Nd,Th:LaAlO3 Shows Promising Potential in High-Energy Pulsed Lasers

The date of: 2022-08-01
viewed: 33
source:azooptics


Pulsed lasers, a crucial component of the laser industry, are continuously developed to produce higher repetition frequencies and greater intensity. Recently published research findings from the Shanghai Institute of Optics and Fine Mechanics at the Chinese Academy of Sciences exhibit a crystal with promising pulsed laser properties. Research efforts led by the group of Professor Yin Hang and published in Optics & Laser Technology have demonstrated the first laser operation of perovskite oxide LaAlO3 doped with 0.1 at% Nd ions and 0.2 at% Th (Nd,Th:LaAlO3).
What are Pulsed Lasers?
Pulsed lasers have been used extensively in a variety of research fields. Some examples include:
Laser micromachining
Interaction of high-field lasers with materials
Biomedical engineering
Optical communications
Laser nuclear fusion
Laser imaging 
Laser pulses are described by their pulse widths, repetition rates, and pulse energies. Short pulse widths and extremely high peak powers of pulsed lasers have benefited the applications above.
The primary materials in high-energy pulsed lasers are rare earth-doped crystalline materials. The high damage threshold of such bulk crystals is conducive to pulsed laser operation.
Theoretically, a longer fluorescence lifetime will result in a higher repetition rate and more pulsed energy output. The output frequency can also be increased by high thermal conductivity.
While several crystals have been used for pulsed lasers, they have had limited success for high energy emission. For example, due to its greater emission cross section and shorter lifetime, Nd: YAG is less effective than doped crystals such as Nd:LuAG and Nd:glass. Because of their structural features, disordered laser crystals such as Ca3Nb1.5Ga3.5O12 are not typically very thermally conductive and are therefore unsuitable for high-energy applications. New crystals must be discovered to satisfy the demands of repeated frequency high-energy lasers.
Crystal Growth and Laser Operation
Professor Yin Hang's research group used the Czochralski method in an iridium crucible to grow a Nd,Th:LaAlO3. A pure LaAlO3 substrate was used as a seed.
ThO2 powders were added to the melt containing high-purity Al2O3, La2O3, Nd2O3,  to achieve doping concentrations of 1 at. % and 0.2 at. %.  The crystal was grown for two days before being cooled for 20 hours at room temperature.
From the base product, domain-free crystals of a particular size are cut for laser use. After cutting and polishing, the crystal maintained a single stable domain, and a 3 mm x 3 mm x 4.5 mm crystal with a domain-free laser face was produced. X-ray diffraction analysis and optical microscopy characterized the Nd and Th co-doped LaAlO3 crystal.
In the laser experimental setup, a straightforward plano-concave cavity construction was used. The pump source used was a fiber-coupled laser diode (LD) with a center wavelength of 793 nm. The Nd,Th:LaAlO3 crystal received the pump light after being focused by a fiber output focusing mirror. An optical spectrum analyzer and a power meter were used to measure the laser's output power and spectrum, respectively.
Absorption and emission data from the experiment show absorption and emission of the pump light at different NIR wavelengths.
Under 793 nm LD excitation, laser operation was realized. Laser output was obtained at a slope efficiency of 36%, and the corresponding optical-to-optical efficiency was at 34%. Laser output efficiency will increase with coating and greater polishing.
Fluorescence lifetime data were also recorded. Up to 317.7 seconds of fluorescence lifespan with a saturated flux of 5 J/cm2 was measured. Nd,Th:LaAlO3 also has higher thermal qualities than neodymium glass thanks to its high thermal conductivity of up to 10.3 W/mK at 25 °C.
Thorium doping stresses the crystal, immobilizing the domain structure. It then selectively slices the crystal to produce a domain-free crystal that extends in the direction of the dopant.
Overall, LaAlO3 is a promising gain medium for high-energy pulsed lasers. Further development and conditioning of the laser control mechanisms should improve the performance of the beam features.



Hot News / Related to recommend
  • 2026 - 10 - 27
    Click on the number of times: 0
    来源:ACS PublicationsRare earth elements are critical to decarbonization, advanced electronics, and defense applications. Traditional hydrometallurgical recovery using liquid–liquid solvent extraction (...
  • 2026 - 10 - 26
    Click on the number of times: 1
    来源:ACS Publications Rare earth elements (REEs) are irreplaceable in advanced new materials and high-end manufacturing industries. However, their nearly identical physicochemical properties, c...
  • 2026 - 10 - 26
    Click on the number of times: 1
    来源:ACS PublicationsThe efficient recovery of rare-earth elements (REEs) from wastewater is crucial for resource utilization and environmental protection. Developing adsorbents with green fabrication p...
  • 2026 - 10 - 23
    Click on the number of times: 2
    来源:Science DirectThe use of rare earth compounds as ceramic coatings to protect engine turbines blades from chemical degradation has been widely studied in the last two decades. After interaction with...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务