Generating ultra-violet lasers with near-infrared light

The date of: 2022-05-20
viewed: 29
Generating ultra-violet lasers with near-infrared light through “domino upconversion” of nanoparticles


 

source:eurekalert

Strong and coherent ultraviolet light emission devices have enormous medical and industrial application potential, but generating ultraviolet light emission in an effective way has been challenging. Recently, a collaborative research team co-led by researchers from City University of Hong Kong (CityU) developed a new approach to generate deep-ultraviolet lasing through a 'domino upconversion' process of nanoparticles using near-infrared light, which is commonly used in telecommunication devices. The findings provide a solution for constructing miniaturised high energy lasers for bio-detection and photonic devices.

In the world of nanomaterials, 'photon upconversion' means that when nanomaterial is excited by light or photons with a long wavelength and low energy, it emits light with a shorter wavelength and higher energy, such as ultraviolet light.

Challenge in achieving photon upconversion

Photon upconversion characterised by high-energy emission upon excitation of lower-energy photons is of exceptional interest among scientists. This is because it holds potential for cost-effective construction of miniaturised deep-ultraviolet emission devices, which have enormous medical and industrial application potential, such as microbial sterilisation and biomedical instrumentation. However, the photon upconversion process has limited flexibility, as it occurs mainly in special lanthanide ions comprising fixed sets of energy levels.

A research team co-led by Professor Wang Feng, from Department of Materials Science and Engineering, and Professor Chu Sai-tak, from Department of Physics at CityU, together with Dr Jin Limin from the Harbin Institute of Technology (Shenzhen), overcame the obstacle by introducing a 'domino upconversion' tactic.

Special structural design of nanopracticles

Domino upconversion is like a chain reaction, in which energy amassed in one upconversion course triggers another succeeding upconversion process. By using a doughnut-shaped microresonator, incorporated with specially designed 'upconversion nanoparticles', the team successfully generated high-energy, deep-ultraviolet light emission at 290nm by excitation of low-energy infrared photons at 1550nm. 

'As the excitation wavelength was in the telecommunication wavelength range, the nanoparticles can be readily used and integrated into existing fibre-optic communication and photonic circuits without complicated modification or adaptation,' said Professor Wang. The findings were published in the journal Nature Communications, titled 'Ultralarge anti-Stokes lasing through tandem upconversion'.

The idea of constructing 'domino upconversion' was inspired by a previous study of energy transfer in core-shell nanoparticles by Professors Wang and Chu. The core-shell structure design of the nanoparticle allows the multiphoton luminescence process in erbium (Er3+) ions. By adapting a similar synthetic protocol, the team successfully constructed 'core-shell-shell' nanoparticles through a wet-chemistry method to explore the energy-transfer mechanism of lanthanide ions, including thulium (Tm3+) ions.

Doughnut-shaped microresonator

Through the careful design of doping composition and concentration in different layers or shells of the upconversion nanoparticles, the team successfully achieved a tandem combination of Er3+ and Tm3+ ions-based upconversion processes (domino upconversion). The Er3+ ions contained in the outer shell responded to 1550 nm near-infrared photon excitation, a wavelength located in the telecommunication range. In the experiment, the team incorporated the nanoparticles into a doughnut-shaped microresonator cavity. Then they excited the nanoparticles with the 1550 nm near-infrared photons, and successfully generated a high-quality ultraviolet microlaser at 289 nm.

'The upconversion nanoparticles act as 'wavelength converters' to multiply the energy of incident infrared photons,' explained Professor Wang. He expects the findings to pave the way for the construction of miniaturised short-wavelength lasers and says they may inspire new ideas for designing photonic circuits. He added that the miniaturised ultraviolet laser using this domino upconversion technology can provide a platform for sensitive bio-detection, such as the detection of cancer cell secretion, by monitoring the lasing intensity and threshold, which offers great biomedical application potential in the future.

The co-first authors of the research are Dr Sun Tianyin and Dr Chen Bing, from the Department of Materials Science and Engineering at CityU. Other team members included Miss Guo Yang, Miss Zhu Qi, Dr Zhao Jianxiong and Dr Li Yuhua from CityU, and researchers from Sun Yat-sen University, Shenzhen University and Harbin Institute of Technology (Shenzhen). This work was supported by the National Natural Science Foundation of China, the Research Grants Council of Hong Kong, and the Shenzhen Fundamental Research Fund.



Hot News / Related to recommend
  • 2026 - 09 - 03
    Click on the number of times: 2
    The Synergistic Impact of Lanthanide-Doped Nickel Iron Sulphides (NiFeSs) Synthesized by a Hydrothermal Method for Effective Water and Urea Electrolysis in Anion Exchange Membranes来源:ACS PublicationsO...
  • 2026 - 09 - 03
    Click on the number of times: 2
    来源:ACS PublicationsMixed valency in compounds containing rare-earth elements can lead to intriguing properties, such as complex magnetism, unique charge transport, and superconductivity. Zintl A14MPn1...
  • 2026 - 09 - 02
    Click on the number of times: 2
    来源:ACS PublicationsEfficient and green separation of rare earth elements (REE) remains a critical challenge, with conventional solvent extraction relying heavily on toxic organic solvents. Herein, thr...
  • 2026 - 09 - 01
    Click on the number of times: 1
    来源:ACS PublicationsRare-earth activation in oxide thin films is often optimized empirically, although excitation-dependent upconversion (UC) is ultimately constrained by the near-surface energetic lan...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务