Rare Earth Elements Await In Waste

The date of: 2022-02-10
viewed: 22
source:Eurasia Review


Rare earth elements are hard to get and hard to recycle, but a flash of intuition led Rice University scientists toward a possible solution. 
The Rice lab of chemist James Tour reports it has successfully extracted valuable rare earth elements (REE) from waste at yields high enough to resolve issues for manufacturers while boosting their profits. 
The lab’s flash Joule heating process, introduced several years ago to produce graphene from any solid carbon source, has now been applied to three sources of rare earth elements — coal fly ash, bauxite residue and electronic waste — to recover rare earth metals, which have magnetic and electronic properties critical to modern electronics and green technologies.
The researchers say their process is kinder to the environment by using far less energy and turning the stream of acid often used to recover the elements into a trickle.
The study appears in Science Advances.                                                             
Rare earth elements aren’t actually rare. One of them, cerium, is more abundant than copper, and all are more abundant than gold. But these 15 lanthanide elements, along with yttrium and scandium, are widely distributed and difficult to extract from mined materials.
“The U.S. used to mine rare earth elements, but you get a lot of radioactive elements as well,” Tour said. “You’re not allowed to reinject the water, and it has to be disposed of, which is expensive and problematic. On the day the U.S. did away with all rare earth mining, the foreign sources raised their price tenfold.”
So there’s plenty of incentive to recycle what’s been mined already, he said. Much of that is piled up or buried in fly ash, the byproduct of coal-fired power plants. “We have mountains of it,” he said. “The residue of burning coal is silicon, aluminum, iron and calcium oxides that form glass around the trace elements, making them very hard to extract.” Bauxite residue, sometimes called red mud, is the toxic byproduct of aluminum production, while electronic waste is from outdated devices like computers and smart phones.   
While industrial extraction from these wastes commonly involves leaching with strong acid, a time-consuming, non-green process, the Rice lab heats fly ash and other materials (combined with carbon black to enhance conductivity) to about 3,000 degrees Celsius (5,432 degrees Fahrenheit) in a second. The process turns the waste into highly soluble “activated REE species.”
Tour said treating fly ash by flash Joule heating “breaks the glass that encases these elements and converts REE phosphates to metal oxides that dissolve much more easily.” Industrial processes use a 15-molar concentration of nitric acid to extract the materials; the Rice process uses a much milder 0.1-molar concentration of hydrochloric acid that still yields more product.
In experiments led by postdoctoral researcher and lead author Bing Deng, the researchers found flash Joule heating coal fly ash (CFA) more than doubled the yield of most of the rare earth elements using very mild acid compared to leaching untreated CFA in strong acids.
“The strategy is general for various wastes,” Bing said. “We proved that the REE recovery yields were improved from coal fly ash, bauxite residue and electronic wastes by the same activation process.” 
The generality of the process makes it especially promising, Bing said, as millions of tons of bauxite residue and electronic waste are also produced every year.
“The Department of Energy has determined this is a critical need that has to be resolved,” Tour said. “Our process tells the country that we’re no longer dependent on environmentally detrimental mining or foreign sources for rare earth elements.”
Tour’s lab introduced flash Joule heating in 2020 to convert coal, petroleum coke and trash into graphene, the single-atom-thick form of carbon, a process now being commercialized. The lab has since adapted the process to convert plastic waste into graphene and to extract precious metals from electronic waste.



Hot News / Related to recommend
  • 2026 - 11 - 17
    Click on the number of times: 0
    来源:Nature CommunicationsLanthanide-doped upconversion nanoparticles exhibit multicolor emission through discrete, narrowband transitions, enabling applications in bioimaging, lasers, and displays. How...
  • 2026 - 11 - 16
    Click on the number of times: 0
    来源:Nature CommunicationsSynergistic spin-state and local coordination engineering offers a promising strategy for enhancing the acidic oxygen reduction reaction performance of Fe-N-C electrocatalysts,...
  • 2026 - 11 - 13
    Click on the number of times: 8
    来源:Nature CommunicationsQuantifying three-dimensional (3D) orientation is critical for understanding self-assembly and collective behavior in soft matter and biological systems. Moreover, orientationa...
  • 2026 - 11 - 12
    Click on the number of times: 11
    来源:Nature CommunicationsRecycling end-of-life (EoL) NdFeB magnets is critical for securing supply of rare-earth element neodymium in the low-carbon transition. We develop a molten salt electrolysis re...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务