The DOE’s Efforts To Extract Rare Earth Minerals From Coal Waste

The date of: 2021-06-01
viewed: 33

source:CleanTechnica

In recent years, the US Department of Energy has been funding a number of pilot plants, where scientists experiment with the best ways to remove valuable rare earth minerals from coal waste. So far, DOE has allocated about $19 million for further research into how much of the valuable materials can be extracted from it. When a technique shows promise, then the site will get additional funding to work toward making the technology work at scale.

So far, plants in Wyoming, West Virginia, North Dakota, Utah, and Kentucky are either under construction or in planning.

“I think we need about three years to develop the technologies and prove them in the field, and then a couple of years to scale up to demonstration scale,” Scott Quillinan, the director of the Center for Economic Geology Research at the University of Wyoming, told Grist. “So I think you’re looking at about the five- to seven-year time scale for commercial deployment.”

There’s a big challenge, though: extracting the rare earths without creating bigger problems than are solved with them.

Laboratories are already pretty good at extracting small amounts of the minerals from coal waste, and at very high purity. Unfortunately, these usually involve creating more pollution, or creating acid waste that’s a net negative. On top of that, it’s very expensive, so nobody ends up winning with current methods.

“We need to find environmentally friendly ways to do this,” Stephan Oborny, a scientist with the Kansas Geological Survey, told Grist. “That’s the tough part.

There’s already a requirement to clean up mining sites, no matter what. Because it’s already being done, it makes a lot more sense to come up with some rare earth minerals in the process. “We’re already actively reclaiming a lot of these abandoned mine sites,” Virginia McLemore, the senior economic geologist for New Mexico’s Bureau of Geology and Mineral Resources told Grist. “If it should be that rare earths are in those wastes, then it becomes attractive.”

As it stands, companies operating the mines already have to pay fees into a mine cleanup fund to cover the cost of cleanup once the mine closes up shop. If the profitable extraction of these metals can be added to the process, a portion of the money from selling them can go toward mine cleanup while the rest benefits whoever is recovering the minerals. This gives everyone incentive to continue the process and helps even more mines get cleaned up.

Towns in coal country that now struggle without the mining and power generation jobs stand to benefit a lot from this arrangement. Instead of shriveling up and dying, or becoming a town of aging (and often sick) retirees without healthcare, these mining towns can do a lot better than the many mining ghost towns that dot the American west. These towns can instead live on in a second wave of benefit from the mines.

The larger benefit comes to the United States as a whole. By recycling these minerals from coal waste (as well as from other types of waste and used products) it can open up an important source of these strategically important metals. They’re not only used in batteries, but also in solar panels, electric motors, and wind turbines. If the US is going to transition away from fossil fuels and toward renewables, it’s going to require a lot more of these minerals than are available on the market today.

Grist says that at present, most of the rare earth mining and production happens in China, and that leaves the US in a strategically bad spot. Relying on a rival country, and one that there are tensions with, for these important minerals is not only bad policy, but could set the transition to renewables back in the future were international relations to worsen.

Clearly, getting this figured out and put into widespread use is going to be a challenge, but it’s a challenge worthy of pursuit. As Grist’s interviewees pointed out, these pilot plants not only stand to make a lot of money selling these valuable minerals, but they also can help fund and promote the cleanup of mining sites. This is definitely a win-win for everyone.

Perhaps more importantly, this gives an opportunity to get rural Americans and Americans from predominantly red states to feel invested in renewables instead of seeing them as the enemy. People who feel like renewables and environmentalism took everything away from them will fight against them. People who feel like they’re being included in the benefits of the process, and people who depend on the process for their family’s future have a lot of incentive to stand with us and promote a transition away from fossil fuels.

This not only helps people (and we at CleanTechnica like people), but it also helps make the situation more politically feasible. If this all works out, it’ll be a huge win.




Hot News / Related to recommend
  • 2026 - 11 - 27
    Click on the number of times: 1
    来源:Scientific ReportsThis study presents a comprehensive investigation into the distribution and recovery of rare earth elements (REEs) throughout the phosphoric acid production process. Analysis of i...
  • 2026 - 11 - 26
    Click on the number of times: 1
    来源:Communications MaterialsIn A2BB'O6 double perovskites (DPs) containing 3d and 5d magnetic ions, the magnetic behavior of the B sublattice can be tuned by choosing nonmagnetic isovalent B' c...
  • 2026 - 11 - 25
    Click on the number of times: 2
    来源:Nature CommunicationsLanthanides serve as essential cofactors in the methanol dehydrogenases of methylotrophic bacteria. While biological function has been characterized for the naturally occurring...
  • 2026 - 11 - 24
    Click on the number of times: 4
    来源:Communications MaterialsConventional polymeric radiation shielding materials suffer from filler aggregation, weak interfacial bonding, and metal leaching. This work presents a chelation immobilizat...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务